Navish M
Navish M
07:54 Jan-12-2009
Lifting Capacity of Yokes

Hello All,

What is the reason behind the lifting capacity of yokes 40lbs on permanent magnet and 10lbs on AC yokes?

Thanks

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
12:27 Jan-12-2009
Re: Lifting Capacity of Yokes
In Reply to Navish M at 07:54 Jan-12-2009 (Opening).

Navish

The requirement of 40lb lift is for DC as well as permanent yokes. DC produces a constant-direction, constant-strength field whereas AC produces a 50 Hz reversing direction and fluctuating-strength field. Have you ever tried lifting MORE than 10lb with an AC yoke, very difficult. Even the 10lb lift needs a well-maintained, flat-footed and deftly handled AC yoke to persistently achieve the lift.

 
 Reply 
 
Sibusiso MZILA
Engineering, Pipeline integrity
Transnet SOC Limited, South Africa, Joined May 2004, 13

Sibusiso MZILA

Engineering, Pipeline integrity
Transnet SOC Limited,
South Africa,
Joined May 2004
13
10:06 Jan-13-2009
Re: Lifting Capacity of Yokes
In Reply to Navish M at 07:54 Jan-12-2009 (Opening).

The major reason for this difference is based on the expected or required depth of penetration; AC has a maximum of 2mm penetration for surface testing whilst DC is expected to penetrate up to 8mm for surface and sub-surface testing.

 
 Reply 
 
Nilesh
Nilesh
13:48 Jan-13-2009
Re: Lifting Capacity of Yokes
In Reply to Navish M at 07:54 Jan-12-2009 (Opening).

Navish Mujawar,
Lifting capacity of yokes are 40 lbs for DC as well as permanent yoke.
Permanent yoke shall have 40 lbs since we are not using any current with it. So fully charged Permanent yoke lift 40 lbs. Due course of time its lifting capacity will drop down in that case you have to send it for re charging. These are used for normally sub surface discontinuities. But for AC as Mr. Nigel explained in one second AC changing its polarity for fifty times. So there is no chance for creating hard magnetic field. and it can lift 10 lbs. Its again gives us better results for surface discontinuities. AC producing magnetic field with sine wave current.
better mobility for particles and lighter penetration in material.

 
 Reply 
 

Product Spotlight

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window