Spot Radiography

Sir,
I want to know
1. What is spot radiography, acceptance criteria for it ?

2. What is ASTM A 516 material ?

3. What is the diff betn. SA 516 Gr. 70 & A 516 Gr.70 material ?

Can u please please send me answer for these?

Regards

Ajit

 
 Reply 
 
bob sudharmin
Engineering, Reliability and Integrity Eng
Shell Malaysia Trading, Malaysia, Joined Jan 2008, 54

bob sudharmin

Engineering, Reliability and Integrity Eng
Shell Malaysia Trading,
Malaysia,
Joined Jan 2008
54
16:45 Feb-08-2009
Re: Spot Radiography
In Reply to AJIT S. PAWAR at 07:51 Feb-08-2009 (Opening).

1. Spot radiography is an aid to quality control where the code does not require a weld to undergo full radiography (100%) . You can make reference to ASME VIII Div 1 UW-11. Acceptance criteria is UW-52
2. ASTM A 516 material is Carbon Steel Pressure Vessel Plates for Moderate and Lower Temperature Service.
3. There is no difference between SA516 Gr 70 and A516 Gr 70 materials. The difference is only in the Grades. ie Gr 65 is different from Gr 70

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 868

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
868
17:17 Feb-08-2009
Re: Spot Radiography
In Reply to bob sudharmin at 16:45 Feb-08-2009 .

Hi Ajit,

To add to Bob's reply, A516 is the ASTM Specification while SA516 is the ASME equivalent.

Mechanical Properties Gr 70:
Tensile: 70 to 90 ksi
Yield: 38 ksi min
Elongation: 17% min in 8” 21% min in 2”

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
21:26 Feb-08-2009
Re: Spot Radiography
In Reply to Michel Couture at 17:17 Feb-08-2009 .

The major difference in Spot vs. 100% RT, other than the coverage, is that in evaluating the image, porosity is not considered. ASME VIII QW-52 vs. QW-51

 
 Reply 
 

Product Spotlight

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window