Circular shot current calculation

Dear All,
as per ASTM for circular shot NI=K/(L/D).
but i am not very clear at the time of calculating L/D for many parts Viz Crankshaft/Camshafts/spindles and other difficult geometry components.
your valuable responce are awaited.

Thanks

Ehsan

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 891

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
891
15:49 Mar-09-2009
Re: Circular shot current calculation
In Reply to Ehsan at 06:11 Mar-09-2009 (Opening).

Ehsan,

Andreas brought a valid point. But one thing I would like to mention to all who do MT is the formulas given in ASTM E709 and E1444 are in my opinion only guidleine or starting point if you will. On factor we never really consider in our calculation is: "permeability".

For this reason, when I taught MT, I used to tell my students the calculations are only a starting point. I would always magnetised my parts using a lower amperage than what my calculation showed me. Always, verify with my pie gauge or QQI to ensure you are getting the proper magnetisation. You will be surprise at how low the amperage is compare to calculations. Other things to consider when doing MT is particle mobility and background.

One other thing, whenever you do MT, try to picture the part as being a straight piece of round stock. You were talking about a crackshaft, well how long would it be if it was straight?

Remember, always verify your magntisation with a QQI or pie gauge.

Cheerio's

I hope this will be of help.

 
 Reply 
 
Andreas
NDT Inspector, Specially in the oilfield
Tuboscope Vetco(Deutschland)Gmbh, Germany, Joined Oct 1999, 131

Andreas

NDT Inspector, Specially in the oilfield
Tuboscope Vetco(Deutschland)Gmbh,
Germany,
Joined Oct 1999
131
19:17 Mar-09-2009
Re: Circular shot current calculation
In Reply to Michel Couture at 15:49 Mar-09-2009 .

The E 709 eveen state that is only a guideline and you should verify the field by a "gausmeter" , correct would be a Tesla meter to use correct SI units.
I like the so called "Burmah-Castrol strip" , it shows you the magnitude and direction of the field.
If you see the three indication on the strip ,the field is 2.4 kA/m or greater (2 - 6 kA/m is required by EN specs).If not placed perpendicular (90° ) to the applied magnetic ,then no indication will be shown.

 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window