Career Discussions
Zaheer
Zaheer
13:01 Mar-07-2009
ASNT UT Level II can perform AUT on welds

Hello
ASNT UT Level II technician can perform AUT on welds(having knowledge on AUT ) with out any additional qualification. Please clarify.

Regards.
Zaheer

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
13:28 Mar-07-2009
Re: ASNT UT Level II can perform AUT on welds
In Reply to Zaheer at 13:01 Mar-07-2009 (Opening).

Hi Zaheer

What is being done for whom, to which Code or standard and what is the customer prepared to acccept. You really dont give enough scenario details for a focused response.

I am certain that many AUT experts hold no qualification, such as the engineers and system designers. Perhaps they may operate systems for trials and demos. If you are referring to production testing leading to accept/reject to a Code then please note the following:

1. Properly it is either SNT-TC-1A Level II or ACCP Lavel II, ASNT Level II is a misconception.

3. ACCP Level II, as far as I know, has no AUT element in its UT qualification process, and so is not applcable for AUT

3. SNT-TC-1A is employer-based, so if the tech has been trained, examined and certified on AUT equipment by the same employer for whom he will be operating the AUT system then the answer is yes. If, say, the tech has not received appropriate AUT training on the equipment, or if the cert is not issued by the tech's current employer, then the answer is "No".

If the tech is working for one of the big AUT companies who has issued the relevant certificate, then I would think that it should be appropriate certification without going in to an audit of their certification system.

Hope this helps

best regards

 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
08:47 Mar-08-2009
Re: ASNT UT Level II can perform AUT on welds
In Reply to Nigel Armstrong at 13:28 Mar-07-2009 .

Dear Zaheer,

Nigel has given a very clear and informative reply. I would like to add only one thing: If I am a customer, I may, in addition, conduct my own audit and ask the Level II to demonstrate his / her competence.

For example, we have taken a hard look at the NDT technicians (whatever their certification may be) when witnessing NDT tests at the customer's place. Similarly, we have asked for a weld coupon even from a qualified welder. May be we were being too cautious, but considering the criticality of items, we were willing to pay for such extra efforts.

With best wishes,

Swamy
Quality and NDT Guru

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 869

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
869
15:55 Mar-08-2009
Re: ASNT UT Level II can perform AUT on welds
In Reply to S.V.Swamy at 08:47 Mar-08-2009 .

Hi Swamy,

You are totally right. It's not being too cautious, but everyone do makes mistake. For some unknown reason, we always see an audit in a negative way. Maybe because the auditor concentrate on our fault and do not praise the good technician! I don't know.

Anyway, we should see an audit as a way to learn. I my view, there is two kinds of people in this world. Those who makes mistake because of a lack of training, understanding and so forth. And those who think they know it all and their way is the only way. In the case of the former, the situation is easely resolved. You train them, you teach them and with understanding, they will correct their mistake. The later, well!!! There isn't much you can do with them, except to show them the door. They are a liability to your company.

 
 Reply 
 
Zaheer
Zaheer
16:44 Mar-08-2009
Re: ASNT UT Level II can perform AUT on welds
In Reply to Michel Couture at 15:55 Mar-08-2009 .

Thanks Mr.Nigel, Swamy, Michel for your valuable guidence

Regards,
Guru.

 
 Reply 
 
F6brat
F6brat
11:15 Mar-09-2009
Re: ASNT UT Level II can perform AUT on welds
In Reply to Zaheer at 13:01 Mar-07-2009 (Opening).

Hi,

I my self work for a multi national company and i have A.I.N.D.T UT Level-2 welds " The Australian equivilent" and i went throught a 3 wekk in-huse training on the runnign of the equipment and systems as you know everyhting is very different when it comes to AUT.

With client Auditing ect... i'v never had a problem and the clients i do this work ofr and very well know Gas, oil & Mining companys.

I sum it up as dont worry about it is it is your employers problem if something goes wrong

 
 Reply 
 

Product Spotlight

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window