3 layer PE - PU foam - PE pipe concentricity measurement

Please help! I am interested in on- line concentricity measurement of the pipe, which consists of 3 layers: PE internal pipe, Polyurethane foam, and PE outside pipe.

Can you advice companies I should contact?

Regards,

Dmitry Ostrovsky


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
09:45 May-28-2001
Re: 3 layer PE - PU foam - PE pipe concentricity measurement
: Please help! I am interested in on- line concentricity measurement of the pipe, which consists of 3 layers: PE internal pipe, Polyurethane foam, and PE outside pipe.
.
: Can you advice companies I should contact?
.
: Regards,
.
: Dmitry Ostrovsky

Refer to "Coextrusion Layer Thickness Measurement"
http://www.ndt.net/article/rohrext/us_coex/us_coe_e.htm

For multilayer foamed PVC pipes the first layer can be measured. The second Layer also, but not
for all thickness and density conditions. Usually be the last (inner) thin PVC layer cannot be measured.

I personally have done tests at Wavin in Germany to solve this problem.
The main problem is that the inner layer interferes with the backwall echo.
I see a little chance to measure the pipe, however the liability is questionable.
You may get better results near the die since the temperature is higher
and sound velocity is low. That means the separation of the inner layer echoes is better.
But all this is not easy and needs a lot of trials.

Rolf Diederichs



 
 Reply 
 
Dr. Patel
R & D, Consultant to Universities/Industries
Fallon Ultrasonics/McMaster University, Canada, Joined May 2001, 20

Dr. Patel

R & D, Consultant to Universities/Industries
Fallon Ultrasonics/McMaster University,
Canada,
Joined May 2001
20
06:20 May-29-2001
Re: 3 layer PE - PU foam - PE pipe concentricity measurement
: Please help! I am interested in on- line concentricity measurement of the pipe, which consists of 3 layers: PE internal pipe, Polyurethane foam, and PE outside pipe.
.
: Can you advice companies I should contact?
.
: Regards,
.
: Dmitry Ostrovsky

We need details on tube and if you have small sample than you can send us. We are supplying number of systems for tube testing for OD ID and ovality and concentricity with very high accuracy. If you are interested than contact us at
Fallon Ultrasonics Inc.
3 Benemar Court, Hamilton, Ontario L8W 2R1
Canada.
.
Regards
Dr. Patel


 
 Reply 
 
Dmitry Ostrovsky
Dmitry Ostrovsky
02:13 May-30-2001
Re: 3 layer PE - PU foam - PE pipe concentricity measurement
I appreciate your comments and suggestions! As far as details on the application, max OD of the inner PE pipe is 110 mm; max OD of the outside PE layer is 162 mm with the wall thickness of the outside layer about 3.5 mm. We are just interested to track how well centered is the inside pipe in polyurethane.

Regards,

Dmitry Ostrovsky


: Please help! I am interested in on- line concentricity measurement of the pipe, which consists of 3 layers: PE internal pipe, Polyurethane foam, and PE outside pipe.
.
: Can you advice companies I should contact?
.
: Regards,
.
: Dmitry Ostrovsky
.



 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window