Dr. Shahid Kabir
, Joined ,
02:36 Mar-23-2009
NDT of post-tensioned bridge decks

My research work aims to overcome the problems related to the assessment of grouted prestress cable ducts in post-tensioned concrete bridge decks, by studying state-of-the-art NDT methods and procedures currently being employed in different applications. The most promising NDT techniques are to be used in the evaluation of samples of post-tensioned concrete elements on a laboratory scale, and subsequently, on selected post-tensioned bridge decks in the field. The evaluations are conducted in order to measure the loss in cross-sectional area of steel strands caused by structural ageing and deterioration in grout-encased pre-stressing tendon in post-tensioned bridge decks.

I am looking for any suggestions for promising NDT techniques to measure the loss in cross-sectional area of steel strands.

 
 Reply 
 
Simon
Simon
15:08 Mar-24-2009
Re: NDT of post-tensioned bridge decks
In Reply to Dr. Shahid Kabir at 02:36 Mar-23-2009 (Opening).

Dear Dr,

I have come across few application datas similar to this on Non Contact Ultrasound Techniques and Digital Radiography.

For Non Contact Ultrasound method, log on to www.ultrangroup.com or write to me for details.

You can browrse the net for Digital RT details or contact us for details if reqd

Simon

 
 Reply 
 
M. Schickert
R & D,
Institute for Materials Research and Testing, Germany, Joined Jan 2000, 18

M. Schickert

R & D,
Institute for Materials Research and Testing,
Germany,
Joined Jan 2000
18
11:29 Mar-26-2009
Re: NDT of post-tensioned bridge decks
In Reply to Dr. Shahid Kabir at 02:36 Mar-23-2009 (Opening).

Dear Dr. Kabir,

extensive research on localizing and analyzing prestressed cable ducts using ultrasound imaging techniques has been conducted, i.e., at our institute (1) and the BAM (2). These methods may be applicable to your problem if there is clear loss over some length. For first references you may search this site or the web using the search terms 'concrete ultrasound' connected with the names 'Schickert' or 'Krause'.

The best method to directly localize cable fractures is probably the magnetic stray field method developed (among others) at TUB (3). They built a large machine for scanning bridge decks. Search this site for 'magnetic concrete' in conjunction with the names 'Hillemeier', 'Scheel', and 'Walther'.

M. Schickert

(1) Institute for Materials Research and Testing at Bauhaus-University Weimar, Weimar, Germany
(2) Federal Institute for Materials Research and Testing, Berlin, Germany
(3) Technical University Berlin, Berlin, Germany

 
 Reply 
 

Product Spotlight

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window