ROBIN
ROBIN
20:56 Mar-29-2009
ASME B 31 CODE CASE 181

IS IT MANDATORY AS PER ASME B31 CODE CASE 181 THAT ALL PHASED ARRAY NDE REPORTS OF PIPING WELDS SHALL BE REVIEWED BY LEVEL 3 INDIVIDUAL.

 
 Reply 
 
Ed T.
Ed T.
23:28 Mar-29-2009
Re: ASME B 31 CODE CASE 181
In Reply to ROBIN at 20:56 Mar-29-2009 (Opening).

I don't see any reference to that in the Code Case that requires a Level III to review reports. It only states the following:

(f) Only Level II or III personnel shall analyze the data or interpret the results.

 
 Reply 
 
R Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

R Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
14:12 Mar-31-2009
Re: ASME B 31 CODE CASE 181
In Reply to Ed T. at 23:28 Mar-29-2009 .

However, like all ASME NDE, the actual procedure [written practice] must be written by a Level III. Assuming the Level II works inside the parameters of an approved procedure and accepts/rejects to the specific criteria in that procedure, he/she requires no further oversight.

 
 Reply 
 
EdT.
EdT.
14:48 Mar-31-2009
Re: ASME B 31 CODE CASE 181
In Reply to R Duwe at 14:12 Mar-31-2009 .

Please provide a reference for your statement. I could not find a requirement for a Level III to write a procedure anywhere in ASME.

In addition, a written Practice is a certification procedure and not an operating procedure.

 
 Reply 
 
Larry Mullins
Consultant
NxtNdT, USA, Joined Apr 2006, 7

Larry Mullins

Consultant
NxtNdT,
USA,
Joined Apr 2006
7
15:32 Mar-31-2009
Re: ASME B 31 CODE CASE 181
In Reply to EdT. at 14:48 Mar-31-2009 .

Gents - perhaps I have an old copy of CC 181 or I am missing something but how does all this reconcile with (from CC 181)

"(j) Examination data including the data record of (c) (mullins - the qual document) above and data analysis or interpretation of (i) above shall be reviewed by a UT level III individual. When flaw evaluation or characterization of (i) (mullins - the data) above are performed by another qualified level II or III individual, their review may be performed by another individual from the same organization. Examination data review shall include verification that the records indicated in Section V, Article 4, T-491 and T-492 and records noted in the applicable Article 4 appendices are available. B31.3, para 346 applies.

Alternatively, the review may be achieved by arranging for a data acquisition and initial interpretation by a Level II individual qualified in accordance with paras. (f) and (h) above, and a final interpretation and evaluation shall be performed by a Level III individual qualified similarly. The Level III individual shall have been qualified in accordance with para. (f) above, including a practical examination on flawed specimens."

Seems like the answer to the original question is - YES assuming we are using PAUT in-lieu of RT i.e.; CC 181)and not merely as an enhancment of plain old Sec V Art 4 UT..

 
 Reply 
 
Ed T.
Ed T.
19:58 Mar-31-2009
Re: ASME B 31 CODE CASE 181
In Reply to Larry Mullins at 15:32 Mar-31-2009 .

I stand correctd. I missed that paragaph. Thanks for the input Larry.

 
 Reply 
 

Product Spotlight

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

GEKKO, Standard and Advanced phased-array for Easier inspection

M2M Gekko® is a field-proven flaw detector offering PAUT, UT, TOFD and TFM through the streamline
...
d user interface Capture™. Released in 32:128, 64:64 or 64:128 channel configurations, Gekko combines high- resolution and speed while reducing inspectors’ training time.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window