Dear all,

Please advice me, What is NDT methode qualification shall be held to conduct Electromagnetic
Inspection ?
And let me know standard code that using

 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
12:39 Apr-13-2009
Re: EMI
In Reply to Kusnadie at 05:37 Apr-13-2009 (Opening).

Kusnadie,
I guess you mean Magnetic Particle Inspection ASNT Level 1 or 2 in MT, or PCN Level 1 or 2 in MT, and it can be done to most Specs ASME, API, ANSI just depends on which code you are working to. But ASME V appendix 6 Methods for Magnetic Particle Examination (MT) should cover you for most things. Hope that has helped you.

Phil

 
 Reply 
 
Bruce McPherson
Consultant
MFL Services, United Kingdom, Joined Mar 2009, 26

Bruce McPherson

Consultant
MFL Services,
United Kingdom,
Joined Mar 2009
26
13:16 Apr-13-2009
Re: EMI
In Reply to Kusnadie at 05:37 Apr-13-2009 (Opening).

Electromagnetic inspection is normally divided in 2 catagories
a. Eddy current inspection - typically performed on non magnetic materials - and commonly used in the inspection of aerospace components and things like thin walled boiler tubes
b. Magnetic flux leakage testing - performed on ferromagnetic materials and most commonly used in the inspection of oilfield tubulars and tank floors
Eddy current inspectors are typically qualified at level 1 or 2 in the ASNT or PCN systems - I'm not sure about which codes and standards are applicable to this method
Magnetic flux leakage testing was recognised as a separate method in SNT-TC-1A 2006 and there is a training syllabus and example questions in htis document. At this time I'm not aware of anyone doing formal training and qualification in the Magnetic flux leakage method although I'll be happy to be corrected on this point
My area of specialisation is the inspection of oilfield tubulars using the MFL method and there are several applicable standards issued by the American Petroleum Institute (API) which address the MFL method including API 5CT, API RP5A5, APIRP-7G-2 etc

Hope this helps

 
 Reply 
 
Abbas Bombaywala
NDT Inspector
Free Lance, India, Joined Jul 2007, 93

Abbas Bombaywala

NDT Inspector
Free Lance,
India,
Joined Jul 2007
93
06:37 Apr-14-2009
Re: EMI
In Reply to Bruce McPherson at 13:16 Apr-13-2009 .

In Reply to Bruce

Well Silverwing is conducting the course for MFL Inspection.

With Regards

 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
10:43 Apr-14-2009
Re: EMI
In Reply to Bruce McPherson at 13:16 Apr-13-2009 .

Thanks Bruce I have not been involved with Eddy Current inspection so this has helped me also.

Regards,

Phil

 
 Reply 
 
ajit rawal
ajit rawal
04:59 Dec-10-2012
Re: Re: EMI
In Reply to Phil at 10:43 Apr-14-2009 .

standard code for EMI is ASTM E-570

 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
10:47 Dec-10-2012
Re: EMI
In Reply to Bruce McPherson at 13:16 Apr-13-2009 .

Eddy curent bsaed inspections are frequently performed on ferritic materails. I know becacuse I have developed equipment for those applications, including "blind" inspection where MPI could not be done without major dismantling.

The FGI technology that I developed well lends itself to mapping the damage at the rail-wheel interface and reveals patterns of damage/defects ot revealed in other ways. It provides other valuable means of condition assessment.

 
 Reply 
 
John Hansen
Director, - Eddy Current Technology
ETher NDE Ltd, United Kingdom, Joined Oct 1999, 73

John Hansen

Director, - Eddy Current Technology
ETher NDE Ltd,
United Kingdom,
Joined Oct 1999
73
12:13 Dec-10-2012
Re: EMI
In Reply to Frank Lund at 10:47 Dec-10-2012 .

You can get PCN certification in Eddy Current weld inspection from most of the training schools in the UK.

Eddy Current Inspection of welds both Ferromagnetic and Non-Ferrromagnetic is covered by the European Standard EN1711:2000. It has particular advantages in inspecting though coated surface (both conductive and non-conductive) and in poor access areas when compared with MPI.

There is more information on our web site here http://www.ethernde.com/probes/weld-probes/discover

 
 Reply 
 

Product Spotlight

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

On-Demand Webinar: Advanced Ultrasonic Techniques for HTHA Detection & Assessment

In the Oil and Gas industry, High Temperature Hydrogen Attack (HTHA) can occur in steels operating a
...
t high temperature, usually above 205°C (400°F). Early stages of HTHA are very difficult to detect. Join us for a webinar presented by Guy Maes, Zetec Sales Engineer Director. The webinar will demonstrate how advanced ultrasonic techniques are deployed for efficient and reliable HTHA inspections.
>