Surface waves on hot steel plates

Dear readers,

I am looking for a way to use surface Rayleigh waves on hot steel plates (150-180 degr. C.)
I am thinking on coupling the sound in the plate by means of a squirter and a high water flow.
The probe is positioned about 3-4 cm above the plate and water flows through the squirter over the plate. Iam not sure this will work specially for the Rayleigh waves travelling over the steel/water boundary?
Has anyone experience with this or other suggestions? please I like to know

 
 Reply 
 
Borja
Director
Innerspec Technologies, USA, Joined Jun 2002, 36

Borja

Director
Innerspec Technologies,
USA,
Joined Jun 2002
36
20:40 Apr-14-2009
Re: Surface waves on hot steel plates
In Reply to Jack Tensen at 17:07 Apr-14-2009 (Opening).

EMAT is a very good option for generating ultrasound on hot materials, and it is especially well suited for generation of guided waves (including surface waves). You can visit www.innerspec.com for additional information.

 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
20:53 Apr-14-2009
Re: Surface waves on hot steel plates
In Reply to Jack Tensen at 17:07 Apr-14-2009 (Opening).

I have never tried the test at high temperature, but at normal environmental temperatures the water on the surface of the metal can be an issue. An incident longitudinal wave in a water column at the correct angle will generate a Rayleigh wave in steel, but the Rayleigh wave will be very quickly dampened by the water on the surface, and not travel very far before dissipating. That may be a problem depending on the specific sensitivity and sound path length requirements of your test.

 
 Reply 
 

Product Spotlight

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>