Dear readers,

I am looking for a way to use surface Rayleigh waves on hot steel plates (150-180 degr. C.)
I am thinking on coupling the sound in the plate by means of a squirter and a high water flow.
The probe is positioned about 3-4 cm above the plate and water flows through the squirter over the plate. Iam not sure this will work specially for the Rayleigh waves travelling over the steel/water boundary?
Has anyone experience with this or other suggestions? please I like to know

 
 Reply 
 
Borja
Director
Innerspec Technologies, USA, Joined Jun 2002, 36

Borja

Director
Innerspec Technologies,
USA,
Joined Jun 2002
36
20:40 Apr-14-2009
Re: Surface waves on hot steel plates
In Reply to Jack Tensen at 17:07 Apr-14-2009 (Opening).

EMAT is a very good option for generating ultrasound on hot materials, and it is especially well suited for generation of guided waves (including surface waves). You can visit www.innerspec.com for additional information.

 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
20:53 Apr-14-2009
Re: Surface waves on hot steel plates
In Reply to Jack Tensen at 17:07 Apr-14-2009 (Opening).

I have never tried the test at high temperature, but at normal environmental temperatures the water on the surface of the metal can be an issue. An incident longitudinal wave in a water column at the correct angle will generate a Rayleigh wave in steel, but the Rayleigh wave will be very quickly dampened by the water on the surface, and not travel very far before dissipating. That may be a problem depending on the specific sensitivity and sound path length requirements of your test.

 
 Reply 
 

Product Spotlight

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

AMIGO2

TSC Amigo2 - ACFM technology has developed a solid reputation for accurately detecting and sizing
...
surface-breaking cracks through paint and coatings. As the industry demands increased performance in speed, signal quality, and portability, it’s time for an evolution. It’s time for Amigo2.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window