UT Question

A question for you UT guys,
We could be reducing a 6m length of s355 250/150?12.5 *6 to 240/150/12.5 (I don't know why they want to do this as we can get this in) How long would it take to UT a section of this?

It will be a single V on both sides.


I'm just looking for an approximate sort of time (give or take what ever probs/set
backs or hassle free) not pin point.

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
03:27 Apr-16-2009
Re: UT Question
My general rule-of-thumb is 1-2 ft/minute, so about 1/2 meter/minute. The 'gotcha!' is that indications take 5-15 minutes each. Thus the time is in the defects found, not the scanning time. I have found enough 'stuff' in 12 meters of weld to keep me busy all day.

If a full formal report of each defect is not required, only marking of the defects and depths, such that the welder can perform repairs, plan on 2-5 minutes per defect.
 
 Reply 
 
Mark
Mark
05:57 Apr-16-2009
Re: UT Question
In Reply to Roger Duwe at 03:27 Apr-16-2009 .

Hi Roger,

I was thinking all day but just wanted to make sure so i'll say 8/10 hrs but could poss be longer all depends on the weld.

Mark

 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window