Dear all,

Can you advise me, how to produce circular magnetic field on test piece which as no acces to
pass through the shooting rod

Test piece that will inspect is threaded guide shoe and float collar.

My facility that available to produce circular magnetic field are shooting rod with CDS and AC Yoke


Regards,

Kusnadie

 
 Reply 
 
Bruce McPherson
Consultant
MFL Services, United Kingdom, Joined Mar 2009, 26

Bruce McPherson

Consultant
MFL Services,
United Kingdom,
Joined Mar 2009
26
13:03 Apr-18-2009
Re: Circular magnetization
In Reply to Kusnadie at 12:28 Apr-18-2009 (Opening).

Kusnadie,
You could try the adjacent conductor method. Place the shooting rod on top of the pipe (make sure it's electrically insulated from the pipe) and then shoot it. Use a Burmah Castrol strip or equivalent to see if there is enough residual circular field to do the inspection. if not shoot the rod again (and again if necessary) until you get enough residual field. Also check how far around the circumference of the pipe the magnetic field is strong enough to do the inspection. This will tell you how many places around the circumference you have to shoot the rod to inspect the full circumference of the pipe.
If you can't get a strong enough magnetic field using this method, then I'm afraid it will have to be the AC yoke

Best Regards

Bruce

 
 Reply 
 
Kusnadie
Kusnadie
14:04 Apr-18-2009
Re: Circular magnetization
In Reply to Bruce McPherson at 13:03 Apr-18-2009 .

Bruce,

Thank you for reply, I will try ASAP

 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window