07:46 Apr-20-2009
C/S Boiler Tube Inspection

Does anyone know of the best way to inspect carbon steel boiler tubes for leaks? These are approximate sizes.
38.1mm OD
31.7mm ID

38.1mm OD
63.5mm ID

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
15:24 Apr-20-2009
Re: C/S Boiler Tube Inspection
In Reply to Ed at 07:46 Apr-20-2009 (Opening).

Hydro test the tubes, prefferably at a pressure greater than the Relief Valve setting. I would go 1-1/4 times PRV setpoint.

Second best is IRIS spinning-head UT inspection. Very slow, thus brutally expensive for a full boiler inspex.

 
 Reply 
 
Dent
Consultant, NDE Manager NDELevel III/3
NDT Consultant, Canada, Joined Nov 1998, 252

Dent

Consultant, NDE Manager NDELevel III/3
NDT Consultant,
Canada,
Joined Nov 1998
252
15:52 Apr-20-2009
Re: C/S Boiler Tube Inspection
In Reply to Roger Duwe at 15:24 Apr-20-2009 .

For gross leaks you may try an air test at low pressure. Use acoustics to listen for leaks.

 
 Reply 
 
Simon
Simon
19:45 Apr-20-2009
Re: C/S Boiler Tube Inspection
In Reply to Ed at 07:46 Apr-20-2009 (Opening).

You can try any of the Ultrasonic Leak Detectors with Ultrasonic Tone Generators to check the leaks in the pipes.

Sonatest has Soundscan units. Check their website

Simon

 
 Reply 
 

Product Spotlight

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window