Tank inspection

I would like to get information on equipment for tank inspection of the latest modification(I am interested in inspection of bottom and walls

Best regards Chairman of the Technical Committee
A.Petrov
WWW.UZK.RU


 
 Reply 
 
Art Leach
Sales
GE Inspection Technologies, USA, Joined Apr 2001, 12

Art Leach

Sales
GE Inspection Technologies,
USA,
Joined Apr 2001
12
07:58 Jun-14-2001
Re: Tank inspection
: I would like to get information on equipment for tank inspection of the latest modification(I am interested in inspection of bottom and walls
.
: Best regards Chairman of the Technical Committee
: A.Petrov
: WWW.UZK.RU
.
If you plan to perfrom Ultrasonic inspections, I suggest you look at the Krautkramer line of Digital Thickness Gauges and in particular the DMS 2 with TopCOAT technology for reading through costings. Krautkramer also offers software for the data recording instruments which allows you to document the results of thickness surveys in the field, transfer data to the computer and print reports.

Contact you local Krautkramer sales representative for additional details....They can be located from the web site directory.

Art.



 
 Reply 
 
Meindert Anderson
Director
Olympus, USA, Joined Dec 1999, 5

Meindert Anderson

Director
Olympus,
USA,
Joined Dec 1999
5
08:29 Jun-14-2001
Re: Tank inspection
You may also check out Panametrics' line of high-end thickness gages for corrosion applications. The 36DL PLUS (with A-Scan) has lots of practical features including Echo-to-Echo, B-Scan with waveform recall, and simultaneous viewing of both live A-Scan and B-Scan. More information, including representation in Russia, is available on the company's website.

Meindert Anderson

: : I would like to get information on equipment for tank inspection of the latest modification(I am interested in inspection of bottom and walls
: .
: : Best regards Chairman of the Technical Committee
: : A.Petrov
: : WWW.UZK.RU
: .
: If you plan to perfrom Ultrasonic inspections, I suggest you look at the Krautkramer line of Digital Thickness Gauges and in particular the DMS 2 with TopCOAT technology for reading through costings. Krautkramer also offers software for the data recording instruments which allows you to document the results of thickness surveys in the field, transfer data to the computer and print reports.
.
: Contact you local Krautkramer sales representative for additional details....They can be located from the web site directory.
.
: Art.
.



 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
02:05 Jun-14-2001
Re: Tank inspection
You are asking a very large question which you need to split up into out of service and on-stream inspection.

You also need to differentiate between standard uninsulated atmospheric tanks, insulated low pressure tanks and non metallic tanks.

Carbon Steel Atmospheric Tanks make up the bulk of the industry and fall under codes such as API 650/653 and EEMUA 159.

In service you can get at shells and roofs to perform UT thickness surveys with a wide range of ultrasonic devices. To avoid scaffolding there is an array of UT and MFL shell crawlers to determine remaining wall.

To determine corrosion activity of tank floors in service you can use Acoustic Emission or In Service Tank Robots. Robots have some limitations and can be expensive.

Once you take a tank out of service you should be looking at some form of overall floor scanning such as MFL or SLOFEC. Statistical coupon cutting or spot ultrasonics is an ineffective method and poses substantial risks of missing problem areas.

This is just a flavour of what needs to be considered



 
 Reply 
 
Christoph Schnitger
Christoph Schnitger
05:10 Jun-17-2001
Re: Tank inspection
You can use the ultrasonic thickness gauge T-Scope III
from Stresstel in addition to the MFL Inspektion in case,
p.ex. you use the MFL Scanner from the company 3P Services
in Lingen.

You find there profile under : http://www.3p-services.com
if you look for new or used ultrasonic equipemnt, such
as T_Scope III from Stresstel ( new equipment ) or such
as Panametrics 26 DL Plus ( used equipment ) please contact
me directly under : schnitger@eure.de

Thanks
C.Schnitger


 
 Reply 
 
MFE Enterprises, Inc.
MFE Enterprises, Inc.
07:01 Jun-19-2001
Re: Tank inspection
MFE Enterprises, Inc. designs, manufactures and sell magnetic flux leakage equipment for the inspection of tank floors. This equipment is adapted to inspect shells in some instances. Please visit our web site at www.mfescan.com to obtain information concerning our products and our company. We will be happy to address any questions you may have via email.


 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>