Thredolet

can anybody tell me what is thredolet, weldolet, sockolet, there difference?
Regards

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
20:17 May-15-2009
Re: Thredolet
In Reply to AJIT P at 12:32 May-15-2009 (Opening).

O'lets are an American invention, from Bonney Forge. They are a family of integrally reinforced branch connections. Thread-o'lets are internally threaded with male NPT. Sock-o'lets have a socket welding opening, and Weld-o'lets are a butt-weld connection. They address the reinforcement necessary to make a branch connection onto a heavy-wall large pipe. Usually a coupling is sufficient for branch openings in STD or Sch 40 pipe, and is usually insufficient on Sch 160. The o'lets are heavy enough that no calculations are required, and no further reinforcement needed.

Please see tha attached web address.

http://www.bonneyforge.com/branch_prod.cfm?id=2

 
 Reply 
 

Product Spotlight

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window