NDT for Composite

I would like to know the best laboratory NDT methods to inspect composite(PMC).

Thank you.


 
 Reply 
 
David
Student, Research Assistant
National University of Malaysia, Malaysia, Joined Jan 2000, 4

David

Student, Research Assistant
National University of Malaysia,
Malaysia,
Joined Jan 2000
4
09:13 Jun-20-2001
Re: NDT for Composite
: I would like to know the best laboratory NDT methods to inspect composite(PMC).
.
: Thank you.
.

Pulse echo ultrasonic method. Normal probe, direct contact.
Frequency range depends on your material thickness also.


 
 Reply 
 
mokhtar
mokhtar
02:36 Jun-21-2001
Re: NDT for Composite
: : I would like to know the best laboratory NDT methods to inspect composite(PMC).
: .
: : Thank you.
: .
.
: Pulse echo ultrasonic method. Normal probe, direct contact.
: Frequency range depends on your material thickness also.
.

Dear Mr David,
What about immersion technique? Let's say a have glass fibre and thickness is 5mm: What frequency should the probe be?

Thank you.


 
 Reply 
 
David
Student, Research Assistant
National University of Malaysia, Malaysia, Joined Jan 2000, 4

David

Student, Research Assistant
National University of Malaysia,
Malaysia,
Joined Jan 2000
4
09:47 Jun-21-2001
Re: NDT for Composite
Immersion technique has its own advantages but the
choice is yours. If the test material can be soaked
into liquid unconditionally, you can proceed with it.
Since your material is relatively thin and considering
that the material is a glass fibre reinforced composite,
the frequency range can be around 0.5MHz to 2MHz.
The selection is fairly at your discretion. Thank you.

All the best, David, N.V.


 
 Reply 
 
A. Mucciardi
Engineering, -
SLX, Inc., USA, Joined Jan 2000, 3

A. Mucciardi

Engineering, -
SLX, Inc.,
USA,
Joined Jan 2000
3
01:37 Jun-21-2001
Re: NDT for Composite
: Immersion technique has its own advantages but the
: choice is yours. If the test material can be soaked
: into liquid unconditionally, you can proceed with it.
: Since your material is relatively thin and considering
: that the material is a glass fibre reinforced composite,
: the frequency range can be around 0.5MHz to 2MHz.
: The selection is fairly at your discretion. Thank you.
.
: All the best, David, N.V.
.

SLX manufactures a tunable filter unit, the Noise Suppressor II, that adds on to any existing UT instrument. The dual tunable Filters (including a PreAmp) can significantly increase the S/N ratio for components possessing either small defects, or highly attenuative grain structure, or both. The NSII comes in four models, each operating in a different, and overlapping, frequency range. One of these models, NSII-L, operates in the 0.5 to 2.4 MHz range which appears to be the band of interest in this application. Details of this inexpensive, add-on instrument can be found at www.SLX-inc.com .

Regards, Tony





 
 Reply 
 
Jeff Leak
Jeff Leak
08:36 Jun-26-2001
Re: NDT for Composite
: I would like to know the best laboratory NDT methods to inspect composite(PMC).
.
: Thank you.


I have been inspection composite materials for about 11 years, at NASA's Marshall Space Flight Center. I typically use 5Mhz, 0.0250"dia probes, in a Type I immersion bath.

Generally, I inspect the composite panels in a thru-transmission mode, looking for the "bulk-attenuation" of the panel. We get a "plan-view" C-Scan image.

Jeff



 
 Reply 
 
Songping Liu
Songping Liu
03:16 Jul-29-2001
Re: NDT for Composite
We have developed a very high resolution RF ultrasonic evaluation technique specially for fiber reinforced composites. It is very useful and smart for applications in laboratory or field for composites.

Thanks

Songping Liu
Ph.D, director of the center for NDT&E
Beijing Aeronautical Manufacturing Technology Research Institute (BAMTRI)
Beijing 100024, P.R. China
E-mail: liusping@public.fhnet.cn.net
Tel: 86-10-65761731-2296(Office)
Fax: 86-10-65762306




 
 Reply 
 
ozan esen
ozan esen
02:08 Dec-18-2002
NDT for Composite
I'm the studen at civil aviation school in Turkey.. Could you please send me some text about "ndt for composites".. thank you..


 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window