Tandem testing of LSAW/Spiral Pipes



I would like to have views regarding tandem testing for mid wall defect in longitudinal/Spiral SAW pipes as per Shell specification (DEP 31.40.20.37 annex d) for automated UT testing in pipe mill. As per the specification we have to use only 45 deg shear wave probe for transmitter and receiver probe. The problem we face is that the reflected angle from inner surface changes depending on the thickness to diameter ratio of pipe and hence to use receiver probe with same angle is not possible. Because of the change in the angle of the returning beam that bounces off the inside diameter of the pipe, the received angle (with respect to the outside surface) will not be the same as the transmitted angle. The skip distance will also change depending on t/D ratio.
As per our trials we have found results are very good with 60/70 deg combination for transmitter and receiver probe depending on t/D ratio of pipe. With 45/45 deg combination we are unable get the results. Why code specs only to use only 45 (± 3) deg probe for both transmitter and receiver?

    
 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1252

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1252
13:44 Jun-15-2009
Re: Tandem testing of LSAW/Spiral Pipes
In Reply to Biju Varghese at 11:36 Jun-15-2009 (Opening).

Biju...API5L is a common standard for Line Pipe and other national and international standards are similar. In the Standard there is no restriction on refracted angle to be 45 degrees. It could be that the person responsible for the company "specification" did not make provision for more effective inspections. API5L in 9.7.4.1 indicates that ANY equipment may be used. However, when used in the pulse-echo mode, it will be very difficult for an operator to correctly position the probes for the midwall region with any angle when required to use the notches or even the through hole because the "maximum amplitude" will generally be from the corner at either the ID or OD. To address this and get midwall coverage, the company I used to work for made a specification to use a calibration standard that used flat bottom holes aligned with the weld centreline in addition to the 1.5mm diameter through hole. Your suggestion for a tandem configuration would be a good option for a "practical solution" to the problem. A description of our concerns in 1998 was made in an article on NDT.net http://www.ndt.net/article/v04n11/eginzel/eginzel.htm
If the client is responsible for setting a specification that limits the efficacy of the guidelines set by the Standard then I would suspect they are also responsible for the outcome.

    
 
 

Product Spotlight

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

XRHRobotStar

In high volume industries like automotive the requirement for a hundred percent X-ray inspection c
...
reates a bottleneck in the production. The XRHRobotStar is a fully Automated Defect Recognition (ADR) capable robot-system that allows an ultra-fast in-line inspection.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window