04:43 Jul-08-2009
UT for bolts

I need UT finding cracks inside the bolts following ASME III NB2580, but in this standard the dia of bolts need to me more than >2". What about the bolts which its diameter <2". How can i check? any one have the procedure about check this caterogy????

 
 Reply 
 
Michael Moles †2014 *1948
, Joined ,
14:30 Jul-08-2009
Re: UT for bolts
In Reply to Creed at 04:43 Jul-08-2009 (Opening).

Yes, Eclipse Scientific Products has technqiues for finding cracks in bolts using phased arrays. Contact them at info@eclipsescientific.com. The technique uses a phased array rotating round the bolt in an encoded jig and an OmniScan.

 
 Reply 
 
Simon
Simon
19:22 Jul-08-2009
Re: UT for bolts
In Reply to Creed at 04:43 Jul-08-2009 (Opening).

You can check with Dakota Ultrasonics. They have Bolt Meter by UT. www.dakotaultrasonics.com - a Group Company of Sonatest Ltd, UK

Simon

 
 Reply 
 

Product Spotlight

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window