04:43 Jul-08-2009
UT for bolts

I need UT finding cracks inside the bolts following ASME III NB2580, but in this standard the dia of bolts need to me more than >2". What about the bolts which its diameter <2". How can i check? any one have the procedure about check this caterogy????

 
 Reply 
 
Michael Moles †2014 *1948
, Joined ,
14:30 Jul-08-2009
Re: UT for bolts
In Reply to Creed at 04:43 Jul-08-2009 (Opening).

Yes, Eclipse Scientific Products has technqiues for finding cracks in bolts using phased arrays. Contact them at info@eclipsescientific.com. The technique uses a phased array rotating round the bolt in an encoded jig and an OmniScan.

 
 Reply 
 
Simon
Simon
19:22 Jul-08-2009
Re: UT for bolts
In Reply to Creed at 04:43 Jul-08-2009 (Opening).

You can check with Dakota Ultrasonics. They have Bolt Meter by UT. www.dakotaultrasonics.com - a Group Company of Sonatest Ltd, UK

Simon

 
 Reply 
 

Product Spotlight

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window