Best In-Service Inspection Technique for Wind Turbine Blades

I'm looking for current information on NDT techniques best suited for inspecting GFRP wind turbine blades in the field. Here's a quick summary of what I've found so far.

-Traditional tap testing is fast, but subjective. Automated tapping methods cover small areas and don't work on thicker laminates.

-Thermography is a great tool that can cover large areas, but is suited for a controlled environment.

-Ultrasound is another great tool, but is time intensive for large areas.

-Acoustic emmision monitoring and vibration analysis are really designed for structural health monitoring (i.e. systems that that installed during construction).

Are there any systems out there right now that are capable of inspecting an entire blade in-service?

 
 Reply 
 
Mr.charles
Mr.charles
04:26 Jul-17-2009
Re: Best In-Service Inspection Technique for Wind Turbine Blades
In Reply to Keith Luscinski at 17:48 Jul-16-2009 (Opening).

It is Charles from Dandong aolong radiative instrument co.,ltd.of China.

We are major in RT equipements manufacture.There is X-ray real-time imaging detetor can be suited for inspecting blades.In china,we have supplies some wind power electric factories to inspect the blades and get a good influence.

If you are interested in it,contact me

E:ndt.charles@gmail.com
F:86-415-6278889
T:
6-415-3458128

 
 Reply 
 
Florin Turcu
R & D
Dept. of Electrical Systems and Automation - University of Pisa, Italy, Joined Jul 2007, 9

Florin Turcu

R & D
Dept. of Electrical Systems and Automation - University of Pisa,
Italy,
Joined Jul 2007
9
18:53 Jul-17-2009
Re: Best In-Service Inspection Technique for Wind Turbine Blades
In Reply to Keith Luscinski at 17:48 Jul-16-2009 (Opening).

Guided waves might work, but I don't know if there's any commercially available tool specific for turbine blades.

 
 Reply 
 
Matt Crompton
Sales, Manager- NDT Sales
Dantec Dynamics Inc, USA, Joined Aug 2008, 3

Matt Crompton

Sales, Manager- NDT Sales
Dantec Dynamics Inc,
USA,
Joined Aug 2008
3
22:15 Jul-17-2009
Re: Best In-Service Inspection Technique for Wind Turbine Blades
In Reply to Keith Luscinski at 17:48 Jul-16-2009 (Opening).

Shearography is both fast, reliable and suitable for in-field inspection. This very week we are conducting in-field trials and are having great success at detecting wrinkles, disbonds, delaminations etc. We are using a portable system and so far the results are very good.

This link has some more info, otherwise please feel free to contact me directly.

http://www.dantecdynamics.com/Default.aspx?ID=2036

 
 Reply 
 
Morgan Troedsson
Consultant, - NDT on FR Composites Wind Blades Aerospace etc.
FORCE Technology, Denmark, Joined Mar 2011, 1

Morgan Troedsson

Consultant, - NDT on FR Composites Wind Blades Aerospace etc.
FORCE Technology,
Denmark,
Joined Mar 2011
1
10:34 Oct-04-2011
Re: Best In-Service Inspection Technique for Wind Turbine Blades
In Reply to Keith Luscinski at 17:48 Jul-16-2009 (Opening).

By far the most reliable NDT technique for FRP composite rotor blades is Ultrasonics (UT). For on-site assessments it may be cumbersome and difficult to handle efficiently by Rope Access or from traditional suspended workin platforms.

Any condition review for MRO on blades should commence with a full blade NDT inspection. Then it is easy to judge and decide on further actions for maintenance: MRO activities up-stairs on installed blade, disassembly of blade for on-site field repair, or eventually bringing the blade to a dedicated MRO workshop.

The key issue is to reach reliability and efficiency in execution of non-destructive condition testing on installed rotor blades. FORCE Technology, in collaboration with PP Techniq, has developed an smart BLADE GUIDED working platform solution (FF360), integrated with a dedicated P-SCAN BLADE SCANNER (AMS-47). The whole system may be operated at regular wind conditions - even up to 14 m/s - with retained safety and efficiency in execution.

Watch our YouTube video presentation on easy handling and installation of the system on installed rotor blades. Watch specifically the sequence with P-scan AMS-47 automated NDT scanner:
http://www.youtube.com/watch?v=J_3Y7iJaOR4

Three rotor blades on a complete turbine may be assessed within a full working day. Even when wind speed is withing normal wind turbine operating condition. That is what we call EFFICIENCY (i.e. without waiting time on the ground).

The technology is viable specifically for multi-MW wind turbines, onshore as well as offshore. You are welcome to contact us for contracts. We may work out an excellent solution for you!

http://www.P-scan.com/

 
 Reply 
 
sudheer jai krishnan
sudheer jai krishnan
18:43 Oct-06-2011
Re: Best In-Service Inspection Technique for Wind Turbine Blades
In Reply to Keith Luscinski at 17:48 Jul-16-2009 (Opening).

Hello Keith,

You can opt for Omniscan MX series from Olympus NDT where Olympus has sold the same Omniscan in huge quantities to many WInd turbine manufacturers around the globe, both for production and for in service applications.

Regards,

S.Sudheer Jai Krishnan

 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window