NDT on Ethylene Pyrolysis furnace tubes

What are the most common NDT methods used to inspect the condition of the tubes? What are the limitations?

Thank you.


 
 Reply 
 
Richard D. Roberts
Engineering, Executive Managment
Quest Integrity Group, USA, Joined Nov 1998, 78

Richard D. Roberts

Engineering, Executive Managment
Quest Integrity Group,
USA,
Joined Nov 1998
78
03:33 Jun-21-2001
Re: NDT on Ethylene Pyrolysis furnace tubes

Dear Sir,

QUEST Integrated, Inc. had developed a "teatherless" (remote) inspection tool, which employs the combined capabilities of high-speed laser and advanced ultrasonic wall thickness measurements. This tool is transported through the piping via a column of clean water, which provides propulsion, a path for the laser beam, and coupling for the ultrasonic signals. The data is processed and stored in the tool using high-speed digital signal processing modules. At the conclusion of an inspection run, the operator downloads the data from the tool to a portable data station. Features such as internal pitting, corrosion, erosion, swelling, and deformation are located and quantitatively mapped. Custom software provides the ability to view the data with contour, cross-sectional, and tabular displays. The furnace tube inspection service (FTIS) is expected to significantly improve both the quality of inspection data and overall safety in the operation of refinery furnaces.

The Furnace Tube Inspection System (FTIS) is a hybrid-technology tool for the inspection furnaces containing 4- to 6- inch (10- to 15-cm) tubing.

The FTIS simultaneously measures: a) Inside radius b) Average radius c) Pit depth d) Wall thickness e) Average wall thickness f) Axial position for all defects.

Advantages Include: a) Performs noncontact in situ measurements, b) Survives harsh hydraulic inspection environments, c) Inspects entire furnace in 15 minutes or less, d) Negotiates one-dimensional (1D) return bends .

You can visit the QUEST web-site at http://www.qi2.com/field/fsddef.htm for additional information or contact me directly.

Regards,
Rich Roberts
--------------- ORIGIONAL MESSAGE -----------
: What are the most common NDT methods used to inspect the condition of the tubes? What are the limitations?
.
: Thank you.
.



 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:09 Jun-30-2001
Re: NDT on Ethylene Pyrolysis furnace tubes
A number of Ethylene Plants apply Acoustic Emission during a hydrotest of the tubes. Activity in the AE occurs from early stages of damage (ie Before the level of ultrasonic detection). Results grade the level of activity in the tubes and they can then be prioritised for other more time consuming inspections such as the Laser, Ultrasonics etc. Good success is reported in A) the speed of the test as all tubes can be tested in one shot B) the ability to identify early stages of damage C) prioritisation and risk ranking for replacement or other inspection work.


 
 Reply 
 

Product Spotlight

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window