13:27 Aug-26-2009
inspection of welding

we find allways after LPI examination of the welding some cracks in de base material.
we want to know what's happend? If somebody can help.

the base material is steel S 235 jr, the electrodes are E7018, the welding process 111

Any information is appreciated.

 
 Reply 
 
Michał
NDT Inspector, Welding Inspector, Mechanical Inspector on behalf of TPI companies
MIDYTEST, Poland, Joined Aug 2007, 14

Michał

NDT Inspector, Welding Inspector, Mechanical Inspector on behalf of TPI companies
MIDYTEST,
Poland,
Joined Aug 2007
14
21:51 Aug-26-2009
Re: inspection of welding
In Reply to fanta diop ndiaye at 13:27 Aug-26-2009 (Opening).

Probably cracks you have mentioned are hydrogen cracks.
Is it possible that you haven't died electrodes enough?
Remember that you absolutly have to dry alkalic electrodes for 1-2 hours in 300-350 C degree.
But I might be wrong - please give some more details if you can.
Best regards
Mike

 
 Reply 
 

Product Spotlight

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window