where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

1205 views
Technical Discussions
Ebrahim Al-Wabary/Saudia Arabia
Ebrahim Al-Wabary/Saudia Arabia
16:04 Sep-12-2009
NDT EQUIPMENT

Gentlemen-----Hi greeting

Please which you recommend to purchase in term of reliabilty,strength,price and accuracy
1. the AGR TD Focus-Scan Phased Array multi channels equipment or Olympos Omniscan Phased Array multi channels equipment?

2. The NDT equipment(except RT equipment) of GE or Olympos or AGR? particularly UT equipment.

Thanks and best regard
Ebrahim Al-Wabary/Saudia Arabia
Mob: +669 504920561
e-mail: wabaryea@Gmail.com

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
14:08 Sep-17-2009
Re: NDT EQUIPMENT
In Reply to Ebrahim Al-Wabary/Saudia Arabia at 16:04 Sep-12-2009 (Opening).

For Phased Array, Omniscan is currently the best of the 'field' instruments.

For manual UT, any of Olympus [Panametrics] or GE [Krautkramer] premier instruments the best available. The software for these two manufacturers is quite a bit different, so it is not easy to go from one brand to another. If you need more than one or two instruments, consider buying all of one brand.

To improve the resolution of manual UT, use only the GE [Krautkramer] composite transducers. Nothing else on the market is even close for resolution and sensitivity.

 
 Reply 
 
Sam
Sam
22:29 Sep-19-2009
Re: NDT EQUIPMENT
In Reply to Roger Duwe at 14:08 Sep-17-2009 .

Basically, as far as I know there are three prominet players namely Ominscan from Olympus, TD Scan from AGR and Phasor from GE. I know it is difficult to lean to one over other, and it is like which car is good GM, Chrysler or Ford.
I am too wondering what are other actual user's thoughts on who has used all three systems in terms its slient technical features, its software, ruggeeness and user friendlyness etc., without any bias on one manufacturer or specifically against one manufactuer.
Sam

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
03:54 Sep-21-2009
Re: NDT EQUIPMENT
In Reply to Sam at 22:29 Sep-19-2009 .

Sam,
I am just familiar with the Omniscan. However, after seeing demonstrations from multiple NDE companies, using a range of PA equipment, both BP (British Petroleum) and Suncor now specify Omniscan as "prequalified". Any other PA system has to be tested and pass a Performance Demonstration, to their satisfaction. I have to respect those opinions, and have drawn some conclusions from the lack of prequalified alternate systems.

 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
17:06 Sep-21-2009
Re: NDT EQUIPMENT
In Reply to Roger Duwe at 03:54 Sep-21-2009 .

Hopefully the conclusions you have drawn relate to the resources that Olympus have allocated to promoting the equipment and supporting evaluations, as well as the excellent job done by some of their technical people (Michael Moles in particular has criss-crossed the world showing people how to solve problems with the Omniscan)

I would not criticise the Olympus equipment itself, but neither would I draw any adverse conclusions about the quality of their competitors equipment.

As always, evaluate the equipment for your situation. Availability of training and support from your local rep are at least as important as the reputation of the system

Joe

 
 Reply 
 

Product Spotlight

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>