metallurgic quiz

Hi everybody....I am studying on metallurgic book because i must do the exam for the second level in FPI and MPI. I have needed of some quiz or question on metallurgic of steel for my two exams. How can you suggest me intenet site or other such as books, ASNT book, etc. for my preparation?
Tanks and best regards..
Aldo

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
02:43 Sep-17-2009
Re: metallurgic quiz
In Reply to aldo at 19:47 Sep-16-2009 (Opening).

Aldo

There should not be many (if any) metallurgy questions in either of those exams - its at 3rd level that a reasonable level of knowledge is expected. And as the exam format is multi-choice (1 right option from 4 or 5) you should be able to discount a 2 or 3 options and then hazard a damned good guess at the remaining 2 options. And if you choose the wrong one, ion a 40 question exam paper you have lost just 2.5%.

However I am all for knowledgable inspectors so here are my 2 recommendations and a bonus:

Google Books has Harry Chandlers "Metallurgy for the non-metallurgist. You can read a good percentage of it on-line for free. OK so you miss some pages but more is on there than is excluded.

If you want a book in your hand then got to http://www.bindt.org/Content.asp?ProdCatID=1&ProdID=16 for Dr Taylor's "Basic Metallurgy for NDT". You cant go wrong with this for just £20!

The bonus is not pure metallurgy but two excellent engineering reads which can be picked up for $10 or less from Amazon are J E Gordon's "New Science of Strong Materials " and "Structures - or why we dont fall through the floor". These should be required reading for everybody concerned with material quality and structural integrity and such fascinating reads as an introduction to materials science with so little maths. The man is a genius educator and polymath who touches on art, history and dress-making on the path to enlightening the layman!

Enjoy your studies and your enthusiam will surely get you through those exams!

 
 Reply 
 

Product Spotlight

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window