water wall corrosion

Can anybody suggest Best Method to detect localised internal corrosion in boilar water wall tubes?
What is the best way to make "mosaic" UT probe? Or is it available in maket ready made? Suggestion Please.

 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
16:28 Sep-27-2009
Re: water wall corrosion
In Reply to sk chaule at 08:33 Sep-27-2009 (Opening).

My first try would be an ultrasonic thickness gauge. If for some reason that doesn't work, I have used radiography. The down side to radiography is, you can't give an exact measurement of the wall thickness, but you can see the corrosion as dark spots on the film.

 
 Reply 
 
John Pursley
R & D
Envision Product Design, USA, Joined Oct 1999, 23

John Pursley

R & D
Envision Product Design,
USA,
Joined Oct 1999
23
08:16 Sep-28-2009
Re: water wall corrosion
In Reply to sk chaule at 08:33 Sep-27-2009 (Opening).

Envision Product Design has developed a digital x-Ray automated boiler waterwall inspection system with backing from EPRI. This system is now ready for commercial application with the 1st prodution unit going to EPRI in October 2009. Http://cmosxray.com

 
 Reply 
 
Slawomir Mackiewicz
Slawomir Mackiewicz
14:36 Sep-28-2009
Re: water wall corrosion
In Reply to sk chaule at 08:33 Sep-27-2009 (Opening).

For reliable detection of localized/pitting corrosion I would suggest application of ultrasonic corrosion mapping system with semi continues thickness data collection and C-scan display of measured wall thickness. There are several systems of this type available on the market. They may be equipped with mechanized, semi mechanized or manual scanners. The main drawback of this type of systems is time consuming scanning.

To overcome this problem when testing large scale objects you can sometimes adopt a statistical approach based on the Statistical Theory of Extreme Values. With this methodology you can obtain quite reliable evaluation of corrosion damage of big structures on the bases of actual scanning of only small fraction (e.q. 2%) of their total area.

 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

NovaScope 6000

The all-digital Novascope 6000 is a portable, ultra-high precision thickness gauge for high-speed
...
thickness measurement. Novascope 6000 has unmatched capabilities and unique features including: •Superior Resolution with high contrast, high-speed color RF display •High pulser voltage •Real-time video output •Increased internal/external data storage •Programmable SetUp features •Battery & AC Powered
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>