ravi prajapati
ravi prajapati
11:22 Sep-28-2009
MPT of Stainless steel

Why Magnetic particle testing is not possible for Stainless steel?

1
 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
12:33 Sep-28-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

most simply put it is not magnetic enough.

1
 
 Reply 
 
Chris Galay
NDT Inspector
Portugal, Joined Sep 2009, 2

Chris Galay

NDT Inspector
Portugal,
Joined Sep 2009
2
23:48 Sep-28-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

The reason why stainless steel cannot be inspected by magnetic particle testing is that we cannot induce a magnetic field on the material as this is non-magnetic. We need a flux leakage so a magnetic field must be present. I hope this will help in your query.

Chris

1
 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
03:10 Sep-29-2009
Re: MPT of Stainless steel
In Reply to anjafo79 at 12:33 Sep-28-2009 .

Its only the austenitic stainless steels which are incapable of magnetisation. The ferritic stainless steels ARE ferromagnetic. Apply a small permanent magnet to the test-piece if you are uncertain whether a material is austenitic or ferritic stainless steel.

2
 
 Reply 
 
Tom Colter
Engineering,
Bechtel Plant Machinery Inc., USA, Joined Nov 1998, 3

Tom Colter

Engineering,
Bechtel Plant Machinery Inc.,
USA,
Joined Nov 1998
3
00:55 Sep-30-2009
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

For a good expalanation of which stainless steels are paramagnetic (can't be subjected to MPT) and which ones are ferromagnetic (can be subjected to MPT) go to this link:
Magnetic Stainless Steel or Not

1
 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
01:17 Sep-30-2009
Re: MPT of Stainless steel
In Reply to Tom Colter at 00:55 Sep-30-2009 .

It is true that you can perform mag particle testing on ferritic stainless steels. The easiest method of determining if the material can be mag particle inspected is to see if a permanent magnet is attracted to it. The three elements which are ferromagnetic are iron, nickel and cobalt.

1
 
 Reply 
 
NIMBANNA
NIMBANNA
07:11 Oct-01-2015
Re: MPT of Stainless steel
In Reply to ravi prajapati at 11:22 Sep-28-2009 (Opening).

All stainless steel materials are nonferrous hence not possible for magnetise the same. For magnetic particle testing, flux leakage is must which is not possible in this case. Hence Magnetic particle testing is not possible. To find out the defects, we may carry out RT / UT which will suffice the requirements.

1
 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
09:26 Oct-01-2015
Re: MPT of Stainless steel
In Reply to NIMBANNA at 07:11 Oct-01-2015 .

Pl. correct your understanding of the subject of stainless steels. All stainless steels are not non-magnetic - ferritic stainless steels and martensitic stainless steels etc. are magnetic. Only austenitic stainless steels in fully annealed condition are non-magnetic (paramagnetic).

Best regards

S V Swamy
Metallurgist and Quality / NDT professional (now retired)

3
 
 Reply 
 
Narayana Prasad.N
Narayana Prasad.N
13:00 Oct-01-2015
Re: MPT of Stainless steel
In Reply to NIMBANNA at 07:11 Oct-01-2015 .

I disagree with your statement that all stainless steels are non ferrous
Regards

3
 
 Reply 
 
Hello Sir
Engineering, welding inspector
Tekfen, India, Joined Sep 2009, 1

Hello Sir

Engineering, welding inspector
Tekfen,
India,
Joined Sep 2009
1
06:47 Feb-20-2017
Re: MPT of Stainless steel
In Reply to Jim Draper at 01:17 Sep-30-2009 .

Hi

Is it possible to perform MPI on Feritic Austenitic steel? pls explain sir

 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
08:42 Feb-20-2017
Re: MPT of Stainless steel
In Reply to Hello Sir at 06:47 Feb-20-2017 .

Ferritic Austenitic Stainless Steels also called duplex steel could be magnetic. As already explained earlier, check whether the material is magnetic or not using a permanent magnet. If the magnet is attracted to the material, MPT is feasible.

Swamy

 
 Reply 
 

Product Spotlight

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window