Concrete NDT and destructive testing

What would be the most common testing (both NDT and destructive testing)methods for pre-cast concrete products. Some methods I can see are the slump test, compression test and hardness tests. What other testing methods are common for this application? Thanks in advance

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
20:09 Oct-08-2009
Re: Concrete NDT and destructive testing
In Reply to Gabriel at 18:32 Oct-08-2009 (Opening).

Gabriel,

I know of the PUNDIT machine for testing concrete. I googled PUNDIT and this led to the present equipment manufacturer, Proceq - they also make the Equotip hardness tester. So go to www.proceq.com for a wide variety of concrete testing electronic equipment.

Cheers

Nigel

 
 Reply 
 
Gabriel
Consultant,
Canada, Joined Oct 2009, 2

Gabriel

Consultant,
Canada,
Joined Oct 2009
2
02:03 Oct-09-2009
Re: Concrete NDT and destructive testing
In Reply to Nigel Armstrong at 20:09 Oct-08-2009 .

Thank you for the information. I had a look at them and it is very useful. Can you think of any other NDT for quality control?

 
 Reply 
 
Ernst Niederleithinger
R & D, -
BAM (Fed. inst. for material research and testing, Germany, Joined Jun 2001, 7

Ernst Niederleithinger

R & D, -
BAM (Fed. inst. for material research and testing,
Germany,
Joined Jun 2001
7
08:18 Oct-09-2009
Re: Concrete NDT and destructive testing
In Reply to Gabriel at 02:03 Oct-09-2009 .

Gabriel,

there are a lot of additional methods (and manufacturers) around. There are eddy current and radar devices e. g. for checking rebar location or acoustic methods (impact echo, ultrasonics) for checking geometry , quality, inhomogeneities.... You can even X-ray.
What is best for you, depends on your application. If you decribe the "precast concrete products" and the problems you expect a little more in detail, I (and others) could recommend suitable methods.

Regards, Ernst

 
 Reply 
 
Martin Schickert
R & D,
Institute for Materials Research and Testing, Germany, Joined Jan 2000, 18

Martin Schickert

R & D,
Institute for Materials Research and Testing,
Germany,
Joined Jan 2000
18
09:28 Oct-09-2009
Re: Concrete NDT and destructive testing
In Reply to Gabriel at 18:32 Oct-08-2009 (Opening).

Gabriel,

the usage of destructive testing methods on pre-cast concrete products depends
1. on the standards applicable to the product in the respective country and
2. on the techniques the manufacturer has found useful for quality control. There is a wide range of possibilies.

Concerning non-destructive methods, I am not aware of any standards. Ultrasonic through transmission has been used for quality control for a long time. Changes of the pulse velocity indicate variations in the manufacturing process, cracks, or other problems.

During the last few years non-destructive testing methods have been developed further. As an example, our institute conducts R&D on ultrasonic methods. It is now possible to measure pulse velocity without surface contact employing air-coupled transducers, or to image concrete elements from one side using electronic and mechanical scanning and 2D or 3D SAFT reconstruction.

Martin Schickert

 
 Reply 
 
Simon Amallraja
Simon Amallraja
14:41 Oct-12-2009
Re: Concrete NDT and destructive testing
In Reply to Gabriel at 18:32 Oct-08-2009 (Opening).

Check the following website: www.ultrangroup.com. They have devloped Non Contact Ultrasonic Systems for Concrete structures like Bridges, Buildings etc.,

Simon

 
 Reply 
 

Product Spotlight

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window