Hi All,

Basically I have an interview on Friday and I know they are having a problem welding inconnel to carbon steel (I don't know the grades, but they are to be used off shore and sub sea), they are having up to 5% dilution problems with the inconnel.

Has anyone ever come across this or a similar problem?

It would be a good topic to talk about at the interview and i'm struggling to find anything from the web

Mark

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
20:44 Oct-20-2009
Re: Cladding Question
In Reply to Mark at 20:13 Oct-20-2009 (Opening).

5% dilution sounds like a submerged-arc SAW overlay. A 'colder' weld process will decrease the dilution. I would try GMAW / MAG in the short-circuiting mode. It has the least penetration, and thus least dilution, of the common welding processes.

 
 Reply 
 
Mark
Mark
21:06 Oct-20-2009
Re: Cladding Question
In Reply to Roger Duwe at 20:44 Oct-20-2009 .

Hi Roger,

Yeah they are using sub arc (I should have said before). They make sub surface christmas trees and apparently spent a fortune on getting 4 very expensive machines so I would imagine they will try like hell to make them viable.

I've only seen pictures of these christmas trees, so i'm not sure if they used MAG and then got these machines to help with the work load or had old sub arc machines there and replaced them.

Not used much sub arc, could polarity be a factor? ie using AC instead of DC?

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
15:40 Oct-21-2009
Re: Cladding Question
In Reply to Mark at 21:06 Oct-20-2009 .

AC is an excellent idea. Hopefully, the new machines have that option.

SAW is run DC-Electrode Positive, putting the bulk of the heat on the wire [and flux pile]. Going to DC-Electrode Negative would put the bulk of the heat onto the base metal, a VERY bad idea. I expect that this would more than double the dilution rate.

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>