transducer backing & matching layers materials

Dear all,

Do someone know where I can find transducer medical backing & matching layers materials data. And where I can buy them?

Best regards,

Didace

 
 Reply 
 
nishal
Consultant, -
University of Strathclyde, United Kingdom, Joined Feb 2008, 2

nishal

Consultant, -
University of Strathclyde,
United Kingdom,
Joined Feb 2008
2
18:39 Oct-22-2009
Re: transducer backing & matching layers materials
In Reply to Didace EKEOM at 17:10 Oct-22-2009 (Opening).

Standard epoxy filled with tungesten partices, is often used as backing for ultrasonic transducers.

Matching layers could be (1) one quarter wavelength layer (2) multiple graded layer configuration. Depending on your configuration, it is just a question of choosing material that has the correct impedance characteristics for your matching layer profile.

nishal

 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window