NDT: SA 578- LEVEL B & C

Dear,
Can any one tell UT as per ASTM-578 which acceptance criteria is more straingent either LEVEL B or LEVEL C?

 
 Reply 
 
GP
Engineering
India, Joined Sep 2009, 2

GP

Engineering
India,
Joined Sep 2009
2
14:31 Oct-28-2009
Re: NDT: SA 578- LEVEL B & C
In Reply to Dhaval Patel at 06:14 Oct-28-2009 (Opening).

Level C is more stringent compared to level B.As per level C,more than 1" continous total loss of back wall reflection plates are rejected.

 
 Reply 
 
Dhaval J patel
Dhaval J patel
04:19 Oct-29-2009
Re: NDT: SA 578- LEVEL B & C
Ref. to my earlier query
Plates acctedpted by Level C can be certified as Level B?
 
 Reply 
 
GP
Engineering
India, Joined Sep 2009, 2

GP

Engineering
India,
Joined Sep 2009
2
09:02 Oct-29-2009
Re: NDT: SA 578- LEVEL B & C
In Reply to Dhaval J patel at 04:19 Oct-29-2009 .

Yes,you can certify as level B.

 
 Reply 
 
CIRO SANTOMARTINO
NDT Inspector,
D.e M.I. srl, Italy, Joined Oct 2009, 86

CIRO SANTOMARTINO

NDT Inspector,
D.e M.I. srl,
Italy,
Joined Oct 2009
86
17:20 Oct-29-2009
Re: NDT: SA 578- LEVEL B & C
In Reply to Dhaval Patel at 06:14 Oct-28-2009 (Opening).

level c. is more straingent .

 
 Reply 
 
R. BALAKUMAR
R. BALAKUMAR
07:02 Nov-14-2012
Re: NDT: SA 578- LEVEL B & C
In Reply to CIRO SANTOMARTINO at 17:20 Oct-29-2009 .

Dear sir,
ASTM A 578 level C or B which is equilent to EN 10160 S1 E1

 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window