00:10 Nov-05-2009
Eddy Current V's DPI/MPI

Would Eddy Current find everything DPI/MPI could?

 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
08:30 Nov-05-2009
Re: Eddy Current V's DPI/MPI
In Reply to anjafo at 00:10 Nov-05-2009 (Opening).

Hi Anjafo,
In theory, Eddy Current should find everything that DPI or MPI will, but there are certain limitations.

MPI is field direction sensitive, so you need to be certain that you have covered the component or area with crossing magnetic fields.
The same is applicable to Eddy Current. This will not easily detect a crack when the probe runs along the length of the crack, so once again, you need to double inspect at right angles to the first inspection to be certain of detecting the cracks.

Also when it comes to borderline defect dimensions, there are some limitations.
In a laboratory environment with experimental Eddy Current equipment, we have been sucessful in reliably detecting cracks of 0.020mm deep, whilst with a very sensitive penetrant or magnetic test, detection of smaller defects could be possible. Here however surface finish is critical for all three methods.

Eddy current can also detect defects under a thin non-conductive coating (like MT, but unlike PT).

Regards,

Godfrey

 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
20:32 Nov-05-2009
Re: Eddy Current V's DPI/MPI
In Reply to Godfrey Hands at 08:30 Nov-05-2009 .

DPI will is not limited to electricaly conductive material. Also, I have used direct current fluorescent MPI to locate flaws 1/4" deep. Of course that is limited to ferromagnetic material, while eddy current can be used to test other electricaly conductive materials.

 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>