gops
gops
09:08 Dec-09-2009
Digital RT

If we use digital radiography in place of conventional RT will there be any improvement in POD to detect tight , underbead & transverse cracks?

 
 Reply 
 
Abbas Bombaywala
NDT Inspector
Free Lance, India, Joined Jul 2007, 94

Abbas Bombaywala

NDT Inspector
Free Lance,
India,
Joined Jul 2007
94
11:40 Dec-09-2009
Re: Digital RT
In Reply to gops at 09:08 Dec-09-2009 (Opening).

Well Gops

In Digital Radiography there are two types

No. 1 Computed Radiography

Computed radiography is a transitional technology between film and direct digital radiography. A reusable, flexible, photo stimulable phosphor (PSP) plate is loaded into a cassette and is exposed in a manner similar to traditional film radiography. The cassette is then placed in a laser reader where it is scanned and translated into a digital image. Depending on the resolution required and image size, the process of digitizing may take from one to five minutes. Once digitally captured, the image may be stored on a computer or other electronic media. Archiving is made easier and the images can be electronically distributed to others for viewing.

This Digital Radiography is used for only the purpose to eliminate use of Films, Chemical & Time of Developing, and it also has advantage of life time storage of data.
So if we talk about this digitzing process I dont think there would be any improvement in POD for any particular defect.

2. Direct Digital Radiography

A direct digital system is different from computed radiography in that it digitizes the photon radiation that passes through an object directly into an image that can be displayed on a computer monitor. Amorphous silicon, charge coupled device (CCD), and complementary metal oxide semiconductor (CMOS) are the three principle technologies used in direct digital imaging. Direct digital system images are available for viewing and analysis in seconds as compared to the minutes required in computed radiography systems. The increased processing speed is a result of the unique construction of the pixels in a direct digital system; an arrangement that also allows an image resolution that is superior to computed radiography and most film applications

In this Direct Digital Radiography yes there is a increase of POD compare to Conventional RT.

I Hope this will help u.

Regards.
Abbas Bombaywala

 
 Reply 
 
gops
gops
12:28 Dec-09-2009
Re: Digital RT
In Reply to Abbas Bombaywala at 11:40 Dec-09-2009 .

Thanks for the feedback.Which one is suitable for large diameter (42")off-shore pipeline erected through barge and whether full panoramic shot is possible with digital radiogrpahy fim holder.

 
 Reply 
 
Abbas Bombaywala
NDT Inspector
Free Lance, India, Joined Jul 2007, 94

Abbas Bombaywala

NDT Inspector
Free Lance,
India,
Joined Jul 2007
94
13:20 Dec-09-2009
Re: Digital RT
In Reply to gops at 12:28 Dec-09-2009 .

Dear Gops

I can't say which one is suitable, but obviously i would go for the technique which has better POD and gives me more Data for ECA.
For More Information u might refer this link http://www.asnt.org/publications/tnt/tnt5-2/tnt5-2fyi.htm.

For Computed Radiography u need the no of cassetes (PSP Plates) to cover your Dia of 42" for a panaromic shots. thats all u need to perform a panaromic shot.

Regards.

 
 Reply 
 
Sashidhar
Sashidhar
18:33 Dec-10-2009
Re: Digital RT
In Reply to gops at 12:28 Dec-09-2009 .

I think Computed radiography can be done on this one. Digital radiography is done in a controlled environment mostly..and for this panoramic shot it may not suit.
Computed radiography can be done easily as long as we have that number of Phosphor plates available.

 
 Reply 
 

Product Spotlight

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window