Corrosion Inspection by UT

Is there any standard/specification regarding UT of corrosion?. I mean, calibration, sensivity setting, and acceptance/rejection criteria.


 
 Reply 
 
Yosi Bar-Cohen
R & D,
Jet Propulsion Lab (JPL), USA, Joined Nov 1998, 26

Yosi Bar-Cohen

R & D,
Jet Propulsion Lab (JPL),
USA,
Joined Nov 1998
26
06:33 Sep-03-1998
Re: Corrosion Inspection by UT
: Is there any standard/specification regarding UT of corrosion?. I mean, calibration, sensivity setting, and acceptance/rejection criteria.

----------

Dear Mr. Pauzi,

There are many standards and specifications for NDE of corrosion
Most of the ones, with which I am familiar, are addressing specific
structures and they are manufacturer proprietary documents. There are
few generic documents that cover standard inspection procedures. As an
example, ASTM has a limited information in its E1004 Standards on Eddy current.

Yosi


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 609

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
609
07:31 Sep-03-1998
Re: Corrosion Inspection by UT
: Is there any standard/specification regarding UT of corrosion?. I mean, calibration, sensivity setting, and acceptance/rejection criteria.

----

Yosi Bar-Cohen mentioned already in his message that you can find standards
addressing certain components.
Here in Germany we have a guideline called US1
'Thickness Measurement with Ultrasound' published by the German Society for NDT,
however so far only in German available,
but I heard that an English version is on the way.

See:
New German guidelines to wall thickness measurement - will be available in English
http://www.ndt.net/news/wt_guid.htm

The handbook contains information on ultrasonic testing of corroded components.
For instance, it is recommended to use an echo display for corrosion gaging since
a blind test is often not reliable enough (digital numbers only).
Also a proper probe characteristic is needed accordingly to the specific geometry
of corrosion. Nowadays are guided waves (lamb waves) used for corrosion testing of
specific structures and depicting the area as an c-scan image without the need to
move the probe (e.g. aircraft structures, pipes).
Examples are aircraft structures and pipes. But since it is a new method I think
there exist no standard yet (Maybe Ahmad Chahbaz knows more about it).

You may also find information browsing/searching NDT.net issue 1997 No. 10 which
focuses on "Ultrasonic Thickness Measurement" http://www.ndt.net/ut1097.htm.

Rolf Diederichs



 
 Reply 
 
Cheryl Simplot
Cheryl Simplot
05:27 Mar-23-1999
Re: Corrosion Inspection by UT
: : Is there any standard/specification regarding UT of corrosion?. I mean, calibration, sensivity setting, and acceptance/rejection criteria.

: ----

: Yosi Bar-Cohen mentioned already in his message that you can find standards
: addressing certain components.
: Here in Germany we have a guideline called US1
: 'Thickness Measurement with Ultrasound' published by the German Society for NDT,
: however so far only in German available,
: but I heard that an English version is on the way.

: See:
: New German guidelines to wall thickness measurement - will be available in English
: http://www.ndt.net/news/wt_guid.htm

: The handbook contains information on ultrasonic testing of corroded components.
: For instance, it is recommended to use an echo display for corrosion gaging since
: a blind test is often not reliable enough (digital numbers only).
: Also a proper probe characteristic is needed accordingly to the specific geometry
: of corrosion. Nowadays are guided waves (lamb waves) used for corrosion testing of
: specific structures and depicting the area as an c-scan image without the need to
: move the probe (e.g. aircraft structures, pipes).
: Examples are aircraft structures and pipes. But since it is a new method I think
: there exist no standard yet (Maybe Ahmad Chahbaz knows more about it).

: You may also find information browsing/searching NDT.net issue 1997 No. 10 which
: focuses on "Ultrasonic Thickness Measurement" http://www.ndt.net/ut1097.htm.

: Rolf Diederichs




 
 Reply 
 

Product Spotlight

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

MIZ®-21C: Truly Affordable Eddy Current Handheld with Surface Array Capability

Introducing MIZ-21C, the first truly affordable handheld eddy current instrument with surface array
...
capabilities. MIZ-21C can deliver fast, accurate inspections in demanding NDT applications including aerospace, oil and gas, manufacturing, and power generation. The surface array solution can reduce inspection time by up to 95% compared to traditional handheld pencil probes. The ergonomic design, long battery life, and intuitive touchscreen mean you can inspect more areas faster than ever without fatigue.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window