where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

11658 views
Technical Discussions
anjafo
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo

NDT Inspector
Norway,
Joined Aug 2009
204
20:16 Dec-15-2009
DAC/AWS/TCG/DGS

Im so used to using a DAC I have forgotten everything mentioned about these other methods on my courses if they where even brought up.

I would like to find out more and if its possible to use some of them in certain cases to improve my inspection methods.

What is each best for?

Type of calibration block for each?

Any literature on the differences?

Thanks in advance.

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
08:49 Dec-19-2009
Re: DAC/AWS/TCG/DGS
In Reply to anjafo at 20:16 Dec-15-2009 (Opening).

Hi Tony

TCG is a time-corrected DAC so that equal dimension reflectors give equal amplitude responses for all sound path distances. Used for PAUT Sectorial scans where it would be otherwise impossible to set every angle and sound path to the same sensitivity level using DAC's.

ASTM E-1316: DGS (distance gain size-German AVG)—distance amplitude curves permitting prediction of reflector size compared to the response from a back surface reflection.

The probe manufacturer supplies data sheet diagams for each probe which shows the amplitude response curves from the backwall and a range of diameters of flat-bottom holes along the length of the soundfield.

Have a look at EN 583-2:2001 Sensitivity and range setting for excellent authoritative descriptions of DAC/TCG and DGS. You'll have to look at AWS D1.1. for instance for knowledge of their sensitivity setting requirements.

Knowledge of these techniques is desirable but will such knowledge really improve your inspection method? You use DAC because the Codes and standards you work to require you to assess indications to those DAC's. A report that a reflector was 3,5 mm equivalent FBH size to DGS would most probably be rejected.

I always liked "Adjust gain until 2mm grass apears acrosss the timebase." and let the technician do the rest in terms of indication characterisation. In my opinion techs raised on this method interrogated the indication envelope (that phrase is almost an anachronism now) the most and built up the best picture of an indication's size, shape and reflecting surfaces. Note even CIT's such as PA and TOFD still often require manual UT characterisation.

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
03:35 Dec-21-2009
Re: DAC/AWS/TCG/DGS
In Reply to Nigel Armstrong at 08:49 Dec-19-2009 .

Ah Nigel, no nostalga for this boy. After I convert a nice, clean DAC curve into a TCG flat-line, life gets very simplified.
"Does the indication break the [flat, straight] reference line?"
if answer is no:
"Does the indication break the nice, straight -12/14dB line?"

I can perform those evaluations 12 hours into a tough day, whiling hanging in a harness, reaching to the back side of a big pipe. Today, most of the tough work is performed during the calibrations. Makes the field measurements & evaluations so very much easier.

 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
15:15 Dec-21-2009
Re: DAC/AWS/TCG/DGS
In Reply to Roger Duwe at 03:35 Dec-21-2009 .

The other applications where TCG has major advantages:

1. automated system - just detect a gate being broken.

2. Highly attenuative materials such as composites or cast iron, where the signal amplitude variation in the region of interest exceeds the 15 dB or so it is practical to evaluate on a constant gain A-scan.

From a code point of view TCG and DAC are effectively equivalent, so you can generally make things a lot easier without a downside. Most codes date back from the days before TCG was such a low cost option, so its rare to find it actually specified.

I have seen instruments that implement a Time controlled gain version of DGS, but I'm not sure about that one.

 
 Reply 
 
Michael Moles †2014 *1948
, Joined ,
15:22 Dec-21-2009
Re: DAC/AWS/TCG/DGS
In Reply to Roger Duwe at 03:35 Dec-21-2009 .

This is exactly why the ASME Code requests a TCG, not a DAC. With a TCG, you can just set your thresold at one pre-defined colour, and everything above it is rejectable; if you want to go -12/-14 dB down from there, you can set your palette accordingly. That way, one can tell at a glance if there is a rejectable defect or not, or a defect that requires further investigation.

Naturally, it is possible to make a DAC (or multiple DACs) for AUT and phased arrays, but there is a LOT more work involved, and a much higher chance of error.

Michael Moles

 
 Reply 
 
adex
adex
17:15 Dec-22-2009
Re: DAC/AWS/TCG/DGS
In Reply to Michael Moles †2014 *1948 at 15:22 Dec-21-2009 .

Hi,

i'm a beginner UT Tech and have a very small experience in Phased array and other advance method. I need your explanation upon your post.

as your post above ;

"This is exactly why the ASME Code requests a TCG, not a DAC."

can you give me the ASME codes for my referrences.


"With a TCG, you can just set your thresold at one pre-defined colour, and everything above it is rejectable; if you want to go -12/-14 dB down from there, you can set your palette accordingly. That way, one can tell at a glance if there is a rejectable defect or not, or a defect that requires further investigation"

I understand but i have a question on +dB and -dB which will represent colour after we set the threshold, is it the +dB and -dB actually represent the amplitudes of the echo because of the setting on Full wave rectifier.

If the answer is NO, what is it?

If the answer is YES, some says that the electric sinusodial graph is not same as ultrasonic pulse wave, is it true ?

If i have wrong information, please correct me.

and lastly, is it true that any equipment that using the colour coding (thresold at one pre-defined colour )for their references need to use TCG???

thank you in advance.

 
 Reply 
 
Michael Moles †2014 *1948
, Joined ,
22:02 Dec-22-2009
Re: DAC/AWS/TCG/DGS
In Reply to adex at 17:15 Dec-22-2009 .

With pleasure. ASME currrently has five Code Cases in Section V Article 4, covering manual and encoded phased array scanning: 2541, 2557, 2558, 2599 and 2600. If you wait until the summer of 2010, we should have a Mandatory Appendix on phased arrays.

There are related practices in ASTM: E-2491 on setting up phased arrays, and E-2700, a procedure for contact weld inspections.

 
 Reply 
 
Krystel
Krystel
07:23 Mar-10-2015
Re: DAC/AWS/TCG/DGS
In Reply to Michael Moles †2014 *1948 at 15:22 Dec-21-2009 .

Michael Moles, what is the uniques advantage of your OmniScan MX2 over other Phased Array Technology?

My colleague is planning to buy phased array equipment.

Thank you.

 
 Reply 
 
Nicholas Bublitz
Other,
VeriPhase, USA, Joined May 2010, 137

Nicholas Bublitz

Other,
VeriPhase,
USA,
Joined May 2010
137
14:00 Mar-10-2015
Re: DAC/AWS/TCG/DGS
In Reply to Krystel at 07:23 Mar-10-2015 .

Krystel
I am with Olympus. My colleague and friend Michael has passed on, so I will answer your query on Olympus' behalf.
I recommend you get a demonstration of the multiple units out in the market and confirm your needs (environment, ease of use, features etc.). We could go on and on about perceived advantages. and another manufacturer will do the same on a forum like this. We do benefit from making the OmniScan platform and being in the phased array game for a long time. You can see the OmniScan page (and our other phased array instruments) here and also sign up for some one to contact you or find your representative on our web page.

http://www.olympus-ims.com/en/phasedarray/
http://www.olympus-ims.com/en/contact-us/

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window