16:46 Dec-27-2009
DGS the simple way

Its been a while since I last used the DGS system for lamination examination of steel plate. Does anyone have a simple explanation of how to go about it. ( an idiots guide)

 
 Reply 
 
Toni Hakkarainen
Director, Technical manager of industrial services
Bureau Veritas Branch Office Finland, Finland, Joined Jun 2006, 4

Toni Hakkarainen

Director, Technical manager of industrial services
Bureau Veritas Branch Office Finland,
Finland,
Joined Jun 2006
4
20:04 Dec-27-2009
Re: DGS the simple way
In Reply to dp_paul_dp at 16:46 Dec-27-2009 (Opening).

If you have a equipment with DGS option, define the reflector type to Back Wall Echo and take the BWE. Thats it.

If you don´t have the DGS option, then you need the printed DGS- curves for your probe. Calibration is similar.

 
 Reply 
 
wasawelder
NDT Inspector
NDT Services, United Kingdom, Joined Dec 2009, 6

wasawelder

NDT Inspector
NDT Services,
United Kingdom,
Joined Dec 2009
6
22:06 Dec-27-2009
Re: DGS the simple way
In Reply to Toni Hakkarainen at 20:04 Dec-27-2009 .

Thanks Toni, trouble is that I don't have a digital set just the old analog, so I really need a step by step guide.

 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
23:36 Dec-27-2009
Re: DGS the simple way
In Reply to wasawelder at 22:06 Dec-27-2009 .

If you don't have a digital set then you MUST have the appropriate curves for the transducer you are using, preferably in the form of a scale for your set.

DGS is a great system, used properly, If you don't use it properly the results can be worse than useless, even with a digital set, In particular, You do need to understand how to compensate for the transfer correction and the material attenuation (which can be significant, especially in shear wave tests) If you don't have the right numbers for this (and for the probe) you wont get the right results.

The Best guide i've come across aimed at technicians is in John Drury's book , Published by Silver Wing, available from them, or from BINDT, as well as many other sources. Its probably still not completely what you are looking for though.

 
 Reply 
 
wasawelder
NDT Inspector
NDT Services, United Kingdom, Joined Dec 2009, 6

wasawelder

NDT Inspector
NDT Services,
United Kingdom,
Joined Dec 2009
6
21:17 Dec-28-2009
Re: DGS the simple way
In Reply to Joe Buckley at 23:36 Dec-27-2009 .

Hi Joe,
Thanks for the reply, I do have a copy of John Drury's book, I'll have to dig it out.
Cheers
paul

 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
00:59 Dec-29-2009
Re: DGS the simple way
In Reply to Joe Buckley at 23:36 Dec-27-2009 .

One point I should add is that if the material to be tested is such that you can use it as a calibration piece (which a piece of plate might well be if it is thick enough that the back surface is out of the near field zone) then the transfer loss can be ignored, and For compression wave testing the material attenuation may also be low enough to ignore.

 
 Reply 
 

Product Spotlight

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window