where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

ULTRASOUND INSTITUTE
The Ultrasound Institute can develop new advanced ultrasonic measurement, imaging and NDT techniques for non-conventional applications.
1812 views
Technical Discussions
junho
NDT Inspector,
KOREA Material INSPECTION, South Korea, Joined Oct 2009, 21

junho

NDT Inspector,
KOREA Material INSPECTION,
South Korea,
Joined Oct 2009
21
07:23 Jan-25-2010
How to use olympus CDS-7t Wedges????

I bought olympus CDS-7t wedge to surface examination. but I don't know how to use
cds- wedge. And I can not find any resources.

I have been using Olympus omniscan-mx. so, omniscan-mx did a lot of bugs?

 
 Reply 
 
junho
NDT Inspector,
KOREA Material INSPECTION, South Korea, Joined Oct 2009, 21

junho

NDT Inspector,
KOREA Material INSPECTION,
South Korea,
Joined Oct 2009
21
08:48 Jan-25-2010
Re: How to use olympus CDS-7t Wedges????
In Reply to junho at 07:23 Jan-25-2010 (Opening).

and How to calibration????

detection and sizing of OD connected cracks is possible ????.

 
 Reply 
 
James Gauthier
Engineering,
ABB, Inc., USA, Joined Nov 2007, 25

James Gauthier

Engineering,
ABB, Inc.,
USA,
Joined Nov 2007
25
15:36 Jan-25-2010
Re: How to use olympus CDS-7t Wedges????
In Reply to junho at 07:23 Jan-25-2010 (Opening).

The OlympusNDT CDS-7t is a great tool to have in your UT Toolbox. It should be coupled with a transducer that is appropriate for the inspection your are attempting. If you want to learn to use this type of probe/wedge combination, I suggest Mark J. Davis (University of Ultrasonics) crack detection course. They will teach you the methods associated with the creeping wave technique as well as other complimentary techniques.

Good Luck!

Jamie

 
 Reply 
 
Michael Moles †2014 *1948
, Joined ,
21:07 Jan-25-2010
Re: How to use olympus CDS-7t Wedges????
In Reply to junho at 07:23 Jan-25-2010 (Opening).

No, the OmniScan MX is relatively bug-free these days. The very early versions had some issues, as do most first generation instruments, but we seem to be running well these days.

If you have problems, contact your Olympus rep or some other expert like one of the training companies for help.

Michael

 
 Reply 
 
Rick Lopez
R & D,
John Deere - Moline Technology Innovation Center, USA, Joined Jul 2011, 191

Rick Lopez

R & D,
John Deere - Moline Technology Innovation Center,
USA,
Joined Jul 2011
191
23:22 Jun-04-2013
Re: How to use olympus CDS-7t Wedges????
In Reply to junho at 07:23 Jan-25-2010 (Opening).

Although this is an old thread, I was recently looking for information about this wedge style myself. I came across a summary by Olympus (Russ Minkwitz) that you may find useful:
http://www.olympus-ims.com/en/applications/detection-sizing-techniques-id-connected-cracking/

 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top