Elastic modulei measurement

Dear All,
it is possible to measure elasticity of a material by UT?
if it is whats the procedure sirs?
regards
rama

 
 Reply 
 
Wieslaw Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 276

Wieslaw Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
276
09:55 Feb-02-2010
Re: Elastic modulei measurement
In Reply to rama at 07:25 Feb-02-2010 (Opening).

It is possible. If you know both sound speeds (longitudinal and transversal waves) and density, you can calculate all elastic parameters (Lame constants) of the material.

There are many possibilities to do it. Ultrasonic refractometry is one of them, spectroscopy methods, combination of acoustical and optical methods (proposed by Bergmann), etc.

 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
14:57 Feb-02-2010
Re: Elastic modulei measurement
In Reply to rama at 07:25 Feb-02-2010 (Opening).

We have an application note on the subject that explains the basic procedure. Please see the link below. As Mr. Bicz write, you need to measure longitudinal and shear (transverse) wave velocity, and know the density of the material, and enter those values into the formula in the app note.

http://www.olympus-ims.com/en/ndt-application/183-id.209715270.html

 
 Reply 
 
ram
NDT Inspector, -
Kuwait, Joined Jan 2010, 13

ram

NDT Inspector, -
Kuwait,
Joined Jan 2010
13
20:08 Feb-02-2010
Re: Elastic modulei measurement
In Reply to Tom Nelligan at 14:57 Feb-02-2010 .

Thank you very much sirs!!!!!!!!!!!!!!
ragards
rama

 
 Reply 
 

Product Spotlight

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>