Dear all,

I want to know what's the affect of pole spacing of yoke if I open the pole too close?

 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 305

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
305
14:55 Feb-06-2010
Re: yoke pole spacing
In Reply to Mulianto Sinaga at 14:38 Feb-06-2010 (Opening).

Hi Mulianto,
If you open the poles up too far, then the magnetic field between the poles may not be enough to detect the cracks you need to find.
If you keep them too close together, there are two risks
1. You will get a smaller coverage, so need to test next test much closer
2. You may saturate with magnetism and cause too big a background to see cracks.

That's a very simple explanation. Hope it helps.

Godfrey

 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
17:23 Feb-06-2010
Re: yoke pole spacing
In Reply to Godfrey Hands at 14:55 Feb-06-2010 .

Mulianto,

I use a Parker DA 200 probe. My manual recomends 5 to 6 inches between the legs. Here is a link to a PDF of the manual. I hope this helps.

http://www.parkreshcorp.com/pdfopinstr/DA200.pdf

 
 Reply 
 
ezio
Other, Retired ex Laboratory Technical Manager
OMECO Research Centre, Italy, Joined Sep 2008, 275

ezio

Other, Retired ex Laboratory Technical Manager
OMECO Research Centre,
Italy,
Joined Sep 2008
275
20:28 Feb-06-2010
Re: yoke pole spacing
In Reply to Mulianto Sinaga at 14:38 Feb-06-2010 (Opening).

You can see the effect with a simple specimen: a plate 50x250x20 mm with a subsurface 1-1,5 mm hole on the side. Good look, ciao, ezio

 
 Reply 
 
rama
NDT Inspector, -
Kuwait, Joined Jan 2010, 13

rama

NDT Inspector, -
Kuwait,
Joined Jan 2010
13
08:59 Feb-07-2010
Re: yoke pole spacing
In Reply to Mulianto Sinaga at 14:38 Feb-06-2010 (Opening).

Pole spacing too close means the magnetic field between the the poles will be greater and it leads to non relevant indications named as banding.

 
 Reply 
 
RENATO BANAGA
Engineering,
Philippine Nuclear Research Institute (PNRI), Philippines, Joined Jul 2005, 8

RENATO BANAGA

Engineering,
Philippine Nuclear Research Institute (PNRI),
Philippines,
Joined Jul 2005
8
11:24 Feb-08-2010
Re: yoke pole spacing
In Reply to rama at 08:59 Feb-07-2010 .

Hi, Mulianto,

Making your Yoke pole spacing too close will create too much sensitivity due to the increase in the magnetic field strenght and that creates unnecessary indications. On the otherhand, making your pole spacing too far would provide lesser magnetic field strenght (lesser sensitivity).
So it is better for you to established your own correct pole spacing by doing some experimentation using same material of the same thickness with a known artificial defect and with that you can make your own appropriate MT procedure.

Renato Banaga

 
 Reply 
 

Product Spotlight

GEKKO, Standard and Advanced phased-array for Easier inspection

M2M Gekko® is a field-proven flaw detector offering PAUT, UT, TOFD and TFM through the streamline
...
d user interface Capture™. Released in 32:128, 64:64 or 64:128 channel configurations, Gekko combines high- resolution and speed while reducing inspectors’ training time.
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window