Prove-up inspection on coated pipe.

A welded SAW pipe with OD/ID coated pipe what would be my distance and v path 1st, 2nd, & 3rd leg in mm? I'm thinking the OD coating is about 18 mm and ID is like paint brush thin.
Epoch unit - 1/2 inch prob 3.5 Mhz. transducer - set up only on a 1/16'' drill hole on.

    
 
 
Ryan Burns
Ryan Burns
08:03 Feb-11-2010
Re: Prove-up inspection on coated pipe.
In Reply to Toni Smith at 04:10 Feb-11-2010 (Opening).

I would hope there are errors in your initial post. First off, I highly doubt you have almost 3/4" of external coating to contend with. Secondly, code compliant shear wave through any discernible volume of coating (or paint) is not an acceptable inspection technique in my experience. Finally....maybe we'd need refracted angle and nominal WT to complete skip distance equations?? If you are the technician why can't you do the math?

    
 
 
Toni Smith
Toni Smith
09:24 Feb-11-2010
Re: Prove-up inspection on coated pipe.
In Reply to Ryan Burns at 08:03 Feb-11-2010 .

What ever I'll do the math. I needed the info because I have been busy doing other things that are important too, thought that u could helped out real quick.

    
 
 

Product Spotlight

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window