14:22 Feb-19-2010
creeping wave methode

hi all

I wondering, Is ASME explaining creeping wave method
for ID deadzone inspect

thank you

 
 Reply 
 
Carlos Correia
R & D, - -
UCV & EGROUP, Venezuela, Joined Oct 2008, 120

Carlos Correia

R & D, - -
UCV & EGROUP,
Venezuela,
Joined Oct 2008
120
19:05 Feb-19-2010
Re: creeping wave methode
In Reply to junho at 14:22 Feb-19-2010 (Opening).

Hello Junho, CW Method is still beyond ASME considerations. You should to check the 2007 edition. But you can write to Ed Ginzel or to Mark Davis. They are part of this forum and is sure they know...

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1286

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1286
19:09 Feb-19-2010
Re: creeping wave methode
In Reply to junho at 14:22 Feb-19-2010 (Opening).

Mr Park
ASME does not describe the "so-called" creeping wave. When you examine the arrival times of the signals when peaking a small depth notch on the opposite wall it will be seen that the detection is actually achieved by the shear headwave. This can be done using a refracted compression mode at some angle between about 70° to 80°
Good description can be found on the application of the techniques in general on http://www.ndt.net/article/pow1297/schmid/schmid.htm

 
 Reply 
 
andrew cunningham
NDT Inspector
Canada, Joined Jun 2008, 238

andrew cunningham

NDT Inspector
Canada,
Joined Jun 2008
238
23:55 Feb-22-2010
Re: creeping wave methode
In Reply to junho at 14:22 Feb-19-2010 (Opening).

Download Mode Change, Creeping Wave or Corner Trap???

Hi Junho

Please find attachment that may explain acoustics of an ID connected reflector.
I hope it helps you.

Yours sincerely
Andrew
 
 Reply 
 

Product Spotlight

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>