Dear collegues,

I am trying to do surface roughness characterization with eddy current probe. Can you advise me about one method that can do this.

Thanking you in advance

Patrick



 
 Reply 
 
Richard D. Finlayson
Director, Operations
Princeton Instruments, USA, Joined Jun 2000, 8

Richard D. Finlayson

Director, Operations
Princeton Instruments,
USA,
Joined Jun 2000
8
02:11 Aug-22-2001
Re: Surface roughness
: Dear collegues,
.
: I am trying to do surface roughness characterization with eddy current probe. Can you advise me about one method that can do this.
.
: Thanking you in advance
.
: Patrick
.

Patrick,
We have developed a system using stress waves that can differentiate between different roughness levels. If you can contact me I can discuss the system further.
Richard



 
 Reply 
 
Dr. Patel
R & D, Consultant to Universities/Industries
Fallon Ultrasonics/McMaster University, Canada, Joined May 2001, 20

Dr. Patel

R & D, Consultant to Universities/Industries
Fallon Ultrasonics/McMaster University,
Canada,
Joined May 2001
20
01:54 Aug-24-2001
Re: Surface roughness
: Dear collegues,
.
: I am trying to do surface roughness characterization with eddy current probe. Can you advise me about one method that can do this.
.
: Thanking you in advance
.
: Patrick

We have developed and used ultrasonic system to measure surface roughness on plates and parts during turning. The system also can measure parts thicknesses in micron accuracy and also measures surface integrity and stresses. If you are interested please contact us at above email.

Regards

Dr. Patel
.



 
 Reply 
 

Product Spotlight

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

On-Demand Webinar: Advanced Ultrasonic Techniques for HTHA Detection & Assessment

In the Oil and Gas industry, High Temperature Hydrogen Attack (HTHA) can occur in steels operating a
...
t high temperature, usually above 205°C (400°F). Early stages of HTHA are very difficult to detect. Join us for a webinar presented by Guy Maes, Zetec Sales Engineer Director. The webinar will demonstrate how advanced ultrasonic techniques are deployed for efficient and reliable HTHA inspections.
>

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window