AxlZ AekZ
AxlZ AekZ
06:49 Aug-20-2001
Can I use coil sensor in DC system?

Can I use coil sensor in DC system for detecting LMA or LF of wire rope?


 
 Reply 
 
Patrick
Patrick
04:13 Aug-20-2001
Re: Can I use coil sensor in DC system?
: Can I use coil sensor in DC system for detecting LMA or LF of wire rope?
.
We know how to test wire rope with eddy current method but what is LMA and LF ?



 
 Reply 
 
Tadeusz Stepinski
R & D
Uppsala University, Sweden, Joined Nov 1998, 14

Tadeusz Stepinski

R & D
Uppsala University,
Sweden,
Joined Nov 1998
14
09:50 Aug-21-2001
Re: Can I use coil sensor in DC system?
: Can I use coil sensor in DC system for detecting LMA or LF of wire rope?
.
You have to give some more details if you want to get some help.


 
 Reply 
 
Alexander Mironenko
Sales,
INTRON PLUS Ltd., Russia, Joined Sep 2001, 17

Alexander Mironenko

Sales,
INTRON PLUS Ltd.,
Russia,
Joined Sep 2001
17
01:52 Sep-10-2001
Re: Can I use coil sensor in DC system?
: : Can I use coil sensor in DC system for detecting LMA or LF of wire rope?
: .
: We know how to test wire rope with eddy current method but what is LMA and LF ?
.
In general you may use coil sensor. LMA - Loss of Metallic cross-sectional Area, LF - Local Flaws (see ASTM 1571-94).



 
 Reply 
 

Product Spotlight

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window