Ketos Ring

dear all!
how do you make the ketos ring? i have Draw( refe to E1444), good mechanic but i have not any information material ? is it low carbon material?
Regard

 
 Reply 
 
Rolf
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf

Director,
NDT.net,
Germany,
Joined Nov 1998
617
19:06 Feb-25-2010
Re: Ketos Ring
In Reply to Trinh Duy Dong at 18:54 Feb-25-2010 (Opening).

I edited your spelling from 'kentos ring' to 'keto ring'. If you search the forum or web for ketos ring you will find better information.

 
 Reply 
 
rafid O. Lopez
rafid O. Lopez
22:58 Feb-25-2010
Re: Ketos Ring
In Reply to Rolf at 19:06 Feb-25-2010 .

Is more easy that you buy the Ring AS5282, is the same that Ketos Ring but wih more sensibility the diference is the annealing. Is difficult to find the ketos ring, and to make it more; many vendors say they sell the ketos ring, but really is the as5282 ring.

Best regards.

 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
16:53 Feb-27-2010
Re: Ketos Ring
In Reply to rafid O. Lopez at 22:58 Feb-25-2010 .

The material is AISI 01 tool steel from annealed round stock, hardness 90 to 95 HRB.

 
 Reply 
 

Product Spotlight

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window