dear all!
how do you make the ketos ring? i have Draw( refe to E1444), good mechanic but i have not any information material ? is it low carbon material?
Regard

 
 Reply 
 
Rolf
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf

Director,
NDT.net,
Germany,
Joined Nov 1998
617
19:06 Feb-25-2010
Re: Ketos Ring
In Reply to Trinh Duy Dong at 18:54 Feb-25-2010 (Opening).

I edited your spelling from 'kentos ring' to 'keto ring'. If you search the forum or web for ketos ring you will find better information.

 
 Reply 
 
rafid O. Lopez
rafid O. Lopez
22:58 Feb-25-2010
Re: Ketos Ring
In Reply to Rolf at 19:06 Feb-25-2010 .

Is more easy that you buy the Ring AS5282, is the same that Ketos Ring but wih more sensibility the diference is the annealing. Is difficult to find the ketos ring, and to make it more; many vendors say they sell the ketos ring, but really is the as5282 ring.

Best regards.

 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
16:53 Feb-27-2010
Re: Ketos Ring
In Reply to rafid O. Lopez at 22:58 Feb-25-2010 .

The material is AISI 01 tool steel from annealed round stock, hardness 90 to 95 HRB.

 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window