About the detecting depth using UT technique for austenitic stainless steel and nickel base alloy

What is the maximum detecting depth? For example,
a 400mm thick plate, material as Incoloy 800H.

 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
09:45 Feb-27-2010
Re: About the detecting depth using UT technique for austenitic stainless steel and nickel base alloy
In Reply to QI at 01:40 Feb-27-2010 (Opening).

Your question is not clear. Did you mean the feasibility of getting a back wall echo from a 400 mm thick Incoloy 800H plate?

If that is what you meant, it is possible using the right probe and instrument combination.

Or are you interested in detecting a discontinuity in such a plate? If this is what you meant, the size of a discontinuity that can be detected depends on several factors including the surface condition, grain size etc. Planar indications of a smaller diameter can be detected compared to spherical / round indications but there can be exceptions too! Since you are discussing a plate, it is expected that both the surfaces are accessible and thus the metal path that needs to be detected is a little more than half the thickness, thus about 250 mm in your case.

If you clarify the question / application, better answers will come.

Regards

 
 Reply 
 
William Blum
Consultant, Training, Level III Services
NDT Consulting Group Inc., USA, Joined Nov 2000, 92

William Blum

Consultant, Training, Level III Services
NDT Consulting Group Inc.,
USA,
Joined Nov 2000
92
10:50 Feb-27-2010
Re: About the detecting depth using UT technique for austenitic stainless steel and nickel base alloy
In Reply to QI at 01:40 Feb-27-2010 (Opening).

You could always take a piece of scrap, create a "defect" like that you must find, then try to find it. If you do that and find the defect you have qualified your procedure.

Bill
NDT Level III
NDT Consulting Group Inc.
www.ndt-cgi.com

 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window