01:40 Feb-27-2010
About the detecting depth using UT technique for austenitic stainless steel and nickel base alloy

What is the maximum detecting depth? For example,
a 400mm thick plate, material as Incoloy 800H.

 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
09:45 Feb-27-2010
Re: About the detecting depth using UT technique for austenitic stainless steel and nickel base alloy
In Reply to QI at 01:40 Feb-27-2010 (Opening).

Your question is not clear. Did you mean the feasibility of getting a back wall echo from a 400 mm thick Incoloy 800H plate?

If that is what you meant, it is possible using the right probe and instrument combination.

Or are you interested in detecting a discontinuity in such a plate? If this is what you meant, the size of a discontinuity that can be detected depends on several factors including the surface condition, grain size etc. Planar indications of a smaller diameter can be detected compared to spherical / round indications but there can be exceptions too! Since you are discussing a plate, it is expected that both the surfaces are accessible and thus the metal path that needs to be detected is a little more than half the thickness, thus about 250 mm in your case.

If you clarify the question / application, better answers will come.

Regards

 
 Reply 
 
William Blum
Consultant, Training, Level III Services
NDT Consulting Group Inc., USA, Joined Nov 2000, 92

William Blum

Consultant, Training, Level III Services
NDT Consulting Group Inc.,
USA,
Joined Nov 2000
92
10:50 Feb-27-2010
Re: About the detecting depth using UT technique for austenitic stainless steel and nickel base alloy
In Reply to QI at 01:40 Feb-27-2010 (Opening).

You could always take a piece of scrap, create a "defect" like that you must find, then try to find it. If you do that and find the defect you have qualified your procedure.

Bill
NDT Level III
NDT Consulting Group Inc.
www.ndt-cgi.com

 
 Reply 
 

Product Spotlight

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window