Technical Discussions
hemant suthar
hemant suthar
09:21 Mar-03-2010
regarding asme sec-ix group no.

what is the purpose of group no. in asme sec-ix and on what base it classified.

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
18:05 Mar-04-2010
Re: regarding asme sec-ix group no.
In Reply to hemant suthar at 09:21 Mar-03-2010 (Opening).

Mr. Suthar, if you mean Group# [versus P#], the Group#'s are subsets of the P#'s that group materials with similar heat-input and heat-treatment characteristics, per ASME Section IX.
Group# is a Supplementary Essential Variable, and is used for controlled heat input Weld Procedures, like when the Impact Strength at Low Temperature is being tested and recorded during the Procedure Qualification.

 
 Reply 
 
Ganesh V
Other, Site Inspection Supervisor
PDO,Oman, India, Joined Jun 2013, 5

Ganesh V

Other, Site Inspection Supervisor
PDO,Oman,
India,
Joined Jun 2013
5
07:19 Jun-07-2013
Re: regarding asme sec-ix group no.
In Reply to hemant suthar at 09:21 Mar-03-2010 (Opening).

Group Numbers are assigned additionally to P-Numbers. These Group Numbers classify the metals within P-Numbers for the purpose of procedure qualification where notch-toughness ( Charpy V-notch impact test ) requirements are specified.
( Refer : QW.200.3 )

So, whenever the codes requires Impact testing, WPS shall specify the Supplimentary essential variables also, and PQR shall reflect the actual p Number's and its applicable Group Numbers, any changes after in WPS need to be requalified with a PQR again.

 
 Reply 
 
Nelson
Nelson
14:21 Sep-18-2013
Re: regarding asme sec-ix group no.
In Reply to Roger Duwe at 18:05 Mar-04-2010 .

Dear Roger Duwe,

Good info you give. How can i refer that it is related with "similar heat input & heat treatment characteristics" in code. i.e, any asme state these group number has been classified according to this? Please reply.
Thanks in advance.

Neo.

 
 Reply 
 
Roger D. Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger D. Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
19:38 Sep-18-2013
Re: regarding asme sec-ix group no.
In Reply to Nelson at 14:21 Sep-18-2013 .

Nelson, that is so basic that the answer is almost hard. This info comes from the definition of "P#" and "Group#". It is part of the foundation of ASME Sect IX. Without it, every different material spec & grade would require its own individualized PQR and WPS.

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window