free software for wavelet analysis and dispersion curve calculation

Hello everybody

free software available:

1) AGU-Vallen Wavelet
In cooperation with Aoyama Gakuin University, Japan, we
developed a software tool to calculate the wavelet transform
from AE signals. The wavelet transform reveals which part of a
signal carries energy at which frequencies. More information can
be found at www.vallen.de/wavelet
We provide this software free of charge to support further
research and development in this field.

*************************
3) Vallen Dispersion
Allows you to calculate the possible wavemodes in a plate,
based on (bulk) longitudinal and transversal speed of sound and
the plate thickness.
This software can be received from www.vallen.de/freeware

regards
Jens Forker



 
 Reply 
 
Nihat
Engineering
Turkey, Joined Jul 2001, 4

Nihat

Engineering
Turkey,
Joined Jul 2001
4
02:52 Aug-22-2001
Re: free software for wavelet analysis and dispersion curve calculation
Jens,

I am working on a project related with wavelet applications in Ultrasonic NDE.
1-Is your software specifically related with AE?
2-Do you have similar softwares which would be applicable for Ultrasonic?

Thanks,
Nihat
GEAE/GE MTC


: Hello everybody
.
: free software available:
.
: 1) AGU-Vallen Wavelet
: In cooperation with Aoyama Gakuin University, Japan, we
: developed a software tool to calculate the wavelet transform
: from AE signals. The wavelet transform reveals which part of a
: signal carries energy at which frequencies. More information can
: be found at www.vallen.de/wavelet
: We provide this software free of charge to support further
: research and development in this field.
.
: *************************
: 3) Vallen Dispersion
: Allows you to calculate the possible wavemodes in a plate,
: based on (bulk) longitudinal and transversal speed of sound and
: the plate thickness.
: This software can be received from www.vallen.de/freeware
.
: regards
: Jens Forker
.



 
 Reply 
 
Christian Grosse
Teacher,
Technische Universität München, Germany, Joined Nov 2000, 11

Christian Grosse

Teacher,
Technische Universität München,
Germany,
Joined Nov 2000
11
03:20 Aug-22-2001
Re: free software for wavelet analysis and dispersion curve calculation
Dear Nihat:

We are developing wavelet based software for applications in Ultrasonic NDE, Impact Echo and Acoustic Emission.

You will find also several articles about similar applications for wavelet transforms in NDE here on NDT.net at:
15th World Conference on Nondestructive Testing
Roma (Italy) 15-21 October 2000 - Proceedings:
http://www.ndt.net/article/wcndt00/index.htm

Regards,
Christian

: Jens,
.
: I am working on a project related with wavelet applications in Ultrasonic NDE.
: 1-Is your software specifically related with AE?
: 2-Do you have similar softwares which would be applicable for Ultrasonic?
.
: Thanks,
: Nihat
: GEAE/GE MTC
.



 
 Reply 
 
Jens Forker
Jens Forker
04:57 Aug-22-2001
Re: free software for wavelet analysis and dispersion curve calculation
Dear Nihat,
the AGU-Vallen Wavelet software can also import ASCII data (from whatever method it comes).
Regards
Jens

: Jens,
.
: I am working on a project related with wavelet applications in Ultrasonic NDE.
: 1-Is your software specifically related with AE?
: 2-Do you have similar softwares which would be applicable for Ultrasonic?
.
: Thanks,
: Nihat
: GEAE/GE MTC
.
.
:
: : Hello everybody
: .
: : free software available:
: .
: : 1) AGU-Vallen Wavelet
: : In cooperation with Aoyama Gakuin University, Japan, we
: : developed a software tool to calculate the wavelet transform
: : from AE signals. The wavelet transform reveals which part of a
: : signal carries energy at which frequencies. More information can
: : be found at www.vallen.de/wavelet
: : We provide this software free of charge to support further
: : research and development in this field.
: .
: : *************************
: : 3) Vallen Dispersion
:: Allows you to calculate the possible wavemodes in a plate,
: : based on (bulk) longitudinal and transversal speed of sound and
: : the plate thickness.
: : This software can be received from www.vallen.de/freeware
: .
: : regards
: : Jens Forker
: .
.



 
 Reply 
 
Maryam Ravan
Maryam Ravan
07:04 Nov-30-2002
Re: free software for wavelet analysis and dispersion curve calculation
: I am working on a project related with wavelet applications in Ultrasonic NDE.
: 1-Is your software specifically related with AE?
: 2-Do you have similar softwares which would be applicable for Ultrasonic?
.
: Thanks,

: Jens,
.
: I am working on a project related with wavelet applications in Ultrasonic NDE.
: 1-Is your software specifically related with AE?
: 2-Do you have similar softwares which would be applicable for Ultrasonic?
.
: Thanks,
: Nihat
: GEAE/GE MTC
.
.
:
: : Hello everybody
: .
: : free software available:
: .
: : 1) AGU-Vallen Wavelet
: : In cooperation with Aoyama Gakuin University, Japan, we
: : developed a software tool to calculate the wavelet transform
: : from AE signals. The wavelet transform reveals which part of a
: : signal carries energy at which frequencies. More information can
: : be found at www.vallen.de/wavelet
: : We provide this software free of charge to support further
: : research and development in this field.
: .
: : *************************
: : 3) Vallen Dispersion
: : Allows you to calculate the possible wavemodes in a plate,
: : based on (bulk) longitudinal and transversal speed of sound and
: : the plate thickness.
: : This software can be received from www.vallen.de/freeware
: .
: : regards
: : Jens Forker
: .
.



 
 Reply 
 
Jens Forker
Jens Forker
08:07 Dec-02-2002
Re: free software for wavelet analysis and dispersion curve calculation
Hi,

AGU-Vallen Wavelet is not specific to AE, virtually all time series data (import filter for ASCII format included, see Helptext) can be processed as the origin of the data is not evaluated. We know that people use it to analyze data from ultrasonics, climate changes (covering centuries), earthquakes,... and many more.

Best regards
Jens Forker

: : I am working on a project related with wavelet applications in Ultrasonic NDE.
: : 1-Is your software specifically related with AE?
: : 2-Do you have similar softwares which would be applicable for Ultrasonic?
: .
: : Thanks,
.
: : Jens,
: .
: : I am working on a project related with wavelet applications in Ultrasonic NDE.
: : 1-Is your software specifically related with AE?
: : 2-Do you have similar softwares which would be applicable for Ultrasonic?
: .
: : Thanks,
: : Nihat
: : GEAE/GE MTC
: .
: .
: :
: : : Hello everybody
: : .
: : : free software available:
: : .
: : : 1) AGU-Vallen Wavelet
: : : In cooperation with Aoyama Gakuin University, Japan, we
: : : developed a software tool to calculate the wavelet transform
: : : from AE signals. The wavelet transform reveals which part of a
: : : signal carries energy at which frequencies. More information can
: : : be found at www.vallen.de/wavelet
: : : We provide this software free of charge to support further
: : : research and development in this field.
: : .
: : : *************************
: : : 3) Vallen Dispersion
: : : Allows you to calculate the possible wavemodes in a plate,
: : : based on (bulk) longitudinal and transversal speed of sound and
: : : the plate thickness.
: : : This software can be received from www.vallen.de/freeware
: : .
: : : regards
: : : Jens Forker
: : .
: .
.



 
 Reply 
 
yew
yew
07:06 Apr-15-2014
Re: free software for wavelet analysis and dispersion curve calculation
In Reply to Jens Forker at 02:45 Aug-22-2001 (Opening).

I have a set data of 1975 numbers of data with the time interval of 2.03E-07. I have used the vallen wavelet to create tra file and the graph shown a straight line. I do have checked on my data and it is correct. In fact, the graph should be showing some peaks instead of straight line. Anyone can help?

 
 Reply 
 
Eraldo Pomponi
R & D, Teaching
Università Politecnica delle Marche, Italy, Joined May 2009, 7

Eraldo Pomponi

R & D, Teaching
Università Politecnica delle Marche,
Italy,
Joined May 2009
7
15:39 Apr-15-2014
Re: free software for wavelet analysis and dispersion curve calculation
In Reply to yew at 07:06 Apr-15-2014 .

Dear Yew,

I don't know Vallen .tra file creator/converter but I would guess that you have a problem with the datatype that, AFAIK, should be int16 and you are probably passing something like float32/float64.
Another option is to move from Vallen software and take your own path with other solutions. There are many other tools out there to perform Wavelet transform. Some examples are:

- Matlab + Wavelet toolbox
- Octave + Wavelab850 (Open Source)
- Python + PyWavelet (Open Source)

HTH,
Eraldo

 
 Reply 
 
Yew Wei Hoe
Yew Wei Hoe
04:28 Apr-16-2014
Re: free software for wavelet analysis and dispersion curve calculation
In Reply to Eraldo Pomponi at 15:39 Apr-15-2014 .

Thanks for the suggestions. The problem is solved. Thank you.

 
 Reply 
 

Product Spotlight

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window