Visibilty of IQI

Is there any possibility of seeing more IQI wire than recommended as per code in X ray radiography, If yes, what are the possibilities?

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
06:41 Mar-15-2010
Re: Visibilty of IQI
In Reply to ezhil at 18:34 Mar-14-2010 (Opening).

Ezhil

Yes, use as low a kV as possible, smallest focal spot size available, maximum source-film distance and slowest film speed available and you will have an excellent but highly uncommercial radiographic image with more wires visible than any Code committee ever dare stipulate.

 
 Reply 
 
Jon Wallis
NDT Inspector, -
Netherlands, Joined Feb 2010, 626

Jon Wallis

NDT Inspector, -
Netherlands,
Joined Feb 2010
626
11:24 Mar-16-2010
Re: Visibilty of IQI
In Reply to Nigel Armstrong at 06:41 Mar-15-2010 .

To continue with Nigels thread....

....and place the IQI on the film side of the object, taped in close contact with the film cassette. You could also use an IQI made of denser material than the material being examined but don't forget to take out the IQI identification tag and replace it with....

You understand that I am NOT being serious. I do wonder though why you would want to produce radiographs of a better than required sensitivity.

 
 Reply 
 

Product Spotlight

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Micro CT

nanoVoxel series has nano-scale resolution by using high voltage X-ray source (from 80-300 kV) wit
...
h micro focal spot and highly sensitive detector including different kinds of big size panel detectors and lens coupling CCD.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window