I want to establish a system that can measure grain size by rayleigh waves.
Is there anybody that help me, how can I measure grain size by this way and
how can establish that experiment setup.
thanks for your helps.


    
 
 Reply 
 
Ernst Niederleithinger
R & D, -
BAM (Fed. inst. for material research and testing, Germany, Joined Jun 2001, 7

Ernst Niederleithinger

R & D, -
BAM (Fed. inst. for material research and testing,
Germany,
Joined Jun 2001
7
01:00 Sep-11-2001
Re: Rayleigh waves
: I want to establish a system that can measure grain size by rayleigh waves.
: Is there anybody that help me, how can I measure grain size by this way and
: how can establish that experiment setup.
: thanks for your helps.

Very interesting. Rayleigh waves are very popular in geophysical/geotechnical testing
(SASW method).
Grain size: R. Chammas (of French streets and bridges authority)
has done FE modelling on the influence of inclusions
on surface waves (rabih.chammas@lcps.fr).
Please keep me informed!





    
 
 Reply 
 
Bruce Maxfield
Engineering, electronics and instrumentation
Analogic Engineering, Inc., USA, Joined Jan 2000, 10

Bruce Maxfield

Engineering, electronics and instrumentation
Analogic Engineering, Inc.,
USA,
Joined Jan 2000
10
01:24 Sep-12-2001
Re: Rayleigh waves
: I want to establish a system that can measure grain size by rayleigh waves.
: Is there anybody that help me, how can I measure grain size by this way and
: how can establish that experiment setup.
: thanks for your helps.
.

I have been working with Fallon Ultrasonics, Inc. on methods to deduce residual stresses from elastic wave velocity measurements. As part of this work, I have used Rayleigh wave ( relatively insensitive to stress) and critically refracted longitudinal wave (much more sensitive to stress) velocities (actually, travel times). These waves have been generated using focused ultrasonic beams like those generated by spherically and cylindrically focused ultrasonic transducers, by plastic wedges of an appropriate angle and by plane waves at an angle to the specimen surface in a water bath. Each of these methods has one or more advantages over the others. In all cases of practical alloys that we have studied, grain scattering is the material parameter that limits the highest frequency that can be used. We have not yet done much quantitative work with respect to determining grain size but it is very clear that the attenuation of these waves is strongly influenced by grain scattering at higher frequencies (as expected) and that this attenuation can be measured with relative ease. There are several corrections that must be made to the measured attenuation in order to obtain the grain scattering term which can be used to deduce the "mean" grain diameter in the region of material being sampled by the elastic wave. If you care to let me know the material and grain size range that is of interest to you, I can give you some general idea of the magnitude of effort that will be required.


    
 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window